SYLGARD 186

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

DOWSIL 186

Main features

  • 10:1 Meter-Mix Processing
  • 255% Cured Elongation
  • 100 ppi Tear Strength

Product Description

SYLGARD 186 Silicone Elastomer combines a two-part, 10:1 mix silicone system with room-temperature and heat-cure options to form a translucent, flexible encapsulant. Its high-viscosity mixed state and 1.65-hour working time support controlled potting and encapsulation of electrical assemblies, including power supplies, sensors, transformers, relays and solar-cell components. After cure, the material combines 255% elongation, 100 ppi Die B tear strength and electrical insulation properties. It can be processed by automated metered mixing and dispensing or by manual mixing, with de-airing selected based on part geometry and process needs.

Key features

  • 10:1 mix ratio: Supports manual or automated metered mixing and dispensing.
  • Flexible cured elastomer: Typical elongation is 255% with Shore A 24 hardness.
  • High tear strength: Typical Die B tear strength is 100 ppi after cure.

Applications

General potting and encapsulation of power supplies, connectors, sensors, controls, transformers, relays and related electrical assemblies.

Technical Specifications

General Properties
Component System
Two (Base / Curing Agent)
Mix Ratio
10:1
Pot Life
1.65 hours
Specific Gravity
1.12
Mechanical Properties
Elongation
255 %
Electrical Properties
Volume Resistivity
4.98 E+15 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the base and mixed material. Values are not specifications.

Property Value Unit Method / condition
Mix ratio 10:1 Base to curing agent
Base viscosity 123800 cP Part A or base
Mixed viscosity 66700 cP Thoroughly mixed material
Working time 1.65 hr At 25 deg C; pot life
Heat-cure time 25 min At 100 deg C
Heat-cure time 15 min At 125 deg C or 150 deg C
Shelf life 12 months Stored at 25 deg C
Technical properties

After-processing / final-state properties

Typical cured properties. Mechanical and electrical values apply to the cured elastomer under the stated test conditions.

Property Value Unit Method / condition
Specific gravity 1.12 Cured material
Tensile strength 305 (2.1) psi (MPa) Typical cured value
Elongation 255 % Typical cured value
Tear strength, Die B 100 (70) ppi (N/cm) Typical cured value
Durometer hardness 24 Shore A Typical cured value
Dielectric constant 2.70 / 2.68 At 100 Hz / 100 kHz
Volume resistivity 4.98E15 ohm cm Typical cured value