LOCTITE STYCAST E2534FR

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE STYCAST E2534FR

Main features

  • Flame retardant
  • Halogen free
  • High thermal conductivity

Product Description

LOCTITE STYCAST E 2534 FR epoxy potting compound complies with recent demands on environmentally friendly products and does not contain brominated flame retardants. It is a two-component epoxy that can be used in a 100:4 ratio with catalysts such as CAT 9. It can achieve a continuous operating temperature of  -40 to 130°C and an intermittent of -40 to 150°C.

LOCTITE STYCAST E 2534 FR can be used with a variety of catalysts. For more information on mixed properties when used with other available catalysts, please contact your local technical service representative for assistance and recommendations.

Recommended Cure Schedule

  • 16 to 24 hours @ 25°C or
  • 2 hour @ 65°C
Product Family

STYCAST E2534FR

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 20 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific Gravity
2.1
Thermal Properties
Glass Transition Temperature (Tg)
76 °C
Thermal Conductivity
1.5 W/m.K
Chemical Properties
Water Absorption
0.03 %
Physical Properties
Viscosity
350,000 mPa.s

Additional Information

What is the difference in viscosity if we use different catalysts?

  • CAT 9 TDS mentions only part A having 350.000 cPs, and no mixed viscosity (estimated around 33.000 cPs)
  • CAT 24LV TDS mentions only the MIXED viscosity around 3.300 cPs, resulting in about 10 times lower viscosity vs CAT 9

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers