Loctite STYCAST 2651-40W1

Harmonization Code : 3907.30.00.15 | Epoxide resin, halogen-free

Loctite STYCAST 2651-40W1

Main features

  • Epoxy Potting and Encapsulation Resin
  • Room-Temperature Encapsulation Cure
  • 0.5 W/(m K) Thermal Encapsulation

Product Description

LOCTITE® STYCAST 2651-40 W1 GOLD is a gold-colored epoxy resin for general potting and encapsulation of metal, plastic, and ceramic assemblies. The material has a typical viscosity of 33,000 mPa·s at 25°C and may be combined with LOCTITE CAT 9 for room-temperature cure or LOCTITE CAT 11 for elevated-temperature cure. The selected catalyst changes mix ratio, pot life, coefficient of thermal expansion, moisture absorption, electrical properties, and operating-temperature range. After cure, the material is documented as machinable with carbide tools.

Key features

  • General potting resin: The epoxy is documented for potting and encapsulation of metals, plastics, and ceramics.
  • Two catalyst options: CAT 9 supports room-temperature cure, while CAT 11 supports elevated-temperature cure.
  • Machinable cured material: The fully cured epoxy may be machined with carbide tools.

Applications / Suitable for

  • General electrical and electronic potting
  • Encapsulation of metal, plastic, and ceramic assemblies
  • Castings requiring post-cure machining
Product Family

STYCAST 2651-40W1

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
Viscosity
32,500 mPa.s
General Properties
Density (g)
1.5 g/cm3
Thermal Properties
Thermal Conductivity
0.55 W/m.K
Electrical Properties
Dielectric Strength
450 kV/mm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or mixed-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Appearance Gold N/A Resin as supplied
Viscosity 33,000 mPa·s At 25°C
Density 1.5 g/cm³ Resin as supplied
Shelf life 365 days At 18°C to 25°C from date of manufacture
Mix ratio with CAT 9 100:8 to 9 parts by weight Resin : catalyst
Pot life with CAT 9 30 min Typical
Mix ratio with CAT 11 100:10 to 11 parts by weight Resin : catalyst
Pot life with CAT 11 4 h Typical
Technical properties

After-processing / final-state properties

Typical final-state values under the stated system and test conditions. These values are not sales specifications.

Property Value Unit Method / condition
Hardness 87.5 Shore D With CAT 9
Thermal conductivity 0.5 W/m·K With CAT 9
CTE 78 ppm/°C With CAT 9
Operating temperature -40 to 175 °C With CAT 9
Hardness 87.5 Shore D With CAT 11
Thermal conductivity 0.5 W/m·K With CAT 11
CTE 45 ppm/°C With CAT 11
Operating temperature -70 to 175 °C With CAT 11

Leading Brands Trust in Our Products and Services