STYCAST 2651-40

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

STYCAST 2651-40

Main features

Product Description

LOCTITE STYCAST 2651-40 CAT 11 is a two-component, heat-curing epoxy encapsulant designed for general-purpose electronic encapsulation applications. This low-viscosity formulation offers excellent adhesion to a wide range of substrates while providing dielectric performance, chemical resistance, and mechanical strength after cure. With a working life exceeding four hours at room temperature and operating temperatures from -55°C to +155°C, it is suitable for encapsulating electronic assemblies, coils, and components that require environmental protection and electrical insulation. The material delivers stable physical and electrical properties in demanding operating environments.

Key features

  • Low viscosity formulation: Mixed viscosity of approximately 4,000 cP supports flow into complex cavities and densely packed assemblies.
  • Dielectric performance: Provides electrical insulation with dielectric strength of 450 volts/mil after cure.
  • Wide temperature capability: Operates across temperatures from -55°C to +155°C for demanding electronic applications.

Applications / Suitable for

Product Family

STYCAST 2651-40

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Black
Chemistry Type
Epoxy
Component System
Two
Density (g)
1.45 g/cm3
Thermal Properties
Operating Temperature
-55 to 155 °C
Thermal Conductivity
0.55 W/m.K
Chemical Properties
Water Absorption
0.1 %
Electrical Properties
Dielectric Strength
17.7 kV/mm

Additional Information

Technical properties

As-supplied / before-processing properties

Properties representative of the uncured resin, catalyst, and mixed system prior to heat cure.

Property Value Unit Method / condition
Mix Ratio 100 : 10.5 Weight Ratio Resin : Catalyst
Mixed Viscosity 4,000 cP Brookfield
Mixed Density 1.45 g/cm³ Mixed material
Working Life >4 hours 100 g mass at 25°C
Shelf Life 6 months Resin at 25°C
Technical properties

After-processing / final-state properties

Representative cured properties following recommended heat cure.

Property Value Unit Method / condition
Shore Hardness 88 Shore D Cured material
Thermal Conductivity 0.55 W/m·K Cured material
Tensile Strength 63 MPa Cured material
Compressive Strength 107 MPa Cured material
Dielectric Strength 450 volts/mil Electrical property
Volume Resistivity >1×10¹⁴ ohm-cm 25°C