STYCAST 1266

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

STYCAST 1266

Main features

  • Low-Viscosity Fine-Gap Impregnation
  • Optically Clear Encapsulation
  • Flexible Ambient or Heat Cure

Product Description

LOCTITE STYCAST 1266 Epoxy Encapsulant is a clear, two-component low-viscosity epoxy system for impregnation and encapsulation where optical clarity and flow into small tolerances are important. Parts A and B mix 100:28 by weight or 100:33 by volume to produce a typical mixed viscosity of 650 cP and a 30-minute working time at 25 deg C. The material can cure at ambient temperature or in one to two hours at 65 deg C, with an optional post-cure. After cure, it provides documented mechanical strength, moisture resistance, and electrical insulation.

Key features

  • Fine-gap impregnation: A typical mixed viscosity of 650 cP supports flow into narrow spaces.
  • Optically clear encapsulation: The clear system supports applications requiring visible components.
  • Flexible cure options: Ambient and heat-cure schedules support different production needs.

Applications

Applications include impregnation and encapsulation of electrical or electronic components, including assemblies with small tolerances and a need for optical clarity.

Product Family

STYCAST 1266

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Component System
Two Part (Resin | Hardener)
Electrical Properties
Dielectric Strength
15.7 kV/mm
Volume Resistivity
1×10¹⁵ Ohms⋅cm
Other Properties
Storage Temperature
25 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Property Value Unit Method / condition
Product form Two-component clear epoxy system Part A is clear amber; Part B is clear yellow
Mix ratio 100:28 parts by weight Part A:Part B
Mix ratio 100:33 parts by volume Part A:Part B
Part A viscosity 8,500 cP ASTM D2393
Part B viscosity 35 cP Typical
Mixed viscosity 650 cP 25 deg C; typical
Mixed specific gravity 1.12 Typical
Working time 30 minutes 100 g mass at 25 deg C
Technical properties

After-processing / final-state properties

Property Value Unit Method / condition
Hardness 75 Shore D ASTM D2240
Dielectric strength 15.7 kV/mm ASTM D149
Dielectric constant 3.0 60 Hz; ASTM D150
Dissipation factor 0.02 60 Hz; ASTM D150
Volume resistivity 1 x 10^15 ohm cm 25 deg C; ASTM D257
Flexural strength 138 N/mm^2 Typical cured value
Compressive strength 69 N/mm^2 Typical cured value
Tensile strength 41 N/mm^2 Typical cured value