STYCAST 1090SI

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

STYCAST 1090SI

Main features

  • High Compressive-Stress Potting
  • Low-Density Deep-Ocean Encapsulation
  • 30-Minute Pot Life

Product Description

LOCTITE STYCAST 1090SI Syntactic Epoxy Encapsulant is a two-component, black syntactic epoxy system for low-density potting under high compressive stress. The 100:11 by-weight resin-to-catalyst mix produces a typical mixed viscosity of 5,000 to 10,000 cP and a 30-minute pot life at 25 deg C. After cure, the material reaches at least 75 Shore D hardness, approximately 65 N/mm^2 compressive strength, and an operating range of -70 to 125 deg C. Its low-density construction and documented deep-ocean use make it suitable for pressure-exposed electrical and electronic encapsulation.

Key features

  • High compressive performance: Typical cured compressive strength is 65 N/mm^2.
  • Low-density syntactic system: A mixed specific gravity of 0.7 to 0.8 supports weight-sensitive potting.
  • Deep-ocean application fit: The product is documented for high-pressure encapsulation environments.

Applications

Applications include deep-ocean and other high-pressure electrical or electronic potting where low density and compressive performance are required.

Product Family

STYCAST 1090SI

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Black
Component System
Two Part (Resin | Hardener)
Pot Life
30 minutes
Specific Gravity
0.7 to 0.8
Thermal Properties
Glass Transition Temperature (Tg)
50 to 60 °C
Operating Temperature
-70 to 125 °C
Electrical Properties
Volume Resistivity
≥1×10¹³ Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Property Value Unit Method / condition
Product form Two-component black syntactic epoxy system Resin and catalyst
Mix ratio 100:11 parts by weight Resin:catalyst
Resin viscosity 30,000-50,000 cP 25 deg C; typical
Mixed viscosity 5,000-10,000 cP 25 deg C; typical
Mixed specific gravity 0.7-0.8 25 deg C; typical
Pot life 30 minutes 25 deg C
Cure schedule 4-24 hours 25 deg C
Post-cure 4 hours at 60-100 deg C May be required for final properties
Technical properties

After-processing / final-state properties

Property Value Unit Method / condition
Operating temperature -70 to 125 deg C Cured material
Coefficient of thermal expansion 58 x 10^-6 K^-1 Typical cured value
Glass transition temperature 50-60 deg C Typical cured range
Thermal conductivity 0.13-0.18 W/(m K) Typical cured range
Hardness >=75 Shore D Typical cured value
Tensile strength 20 N/mm^2 Typical cured value
Compressive strength 65 N/mm^2 Typical cured value
Volume resistivity >=1 x 10^13 ohm cm Typical cured value