TIP 3500 | Thermal insulator pad

Harmonization Code : 3824.99.96.99 | Prepared binders for foundry moulds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included : Other : Other: Other

TIP3500 | Thermal insulator pad

Main features

  • 0.18 - 0.23 Thermal Impedance
  • 3.5 Thermal Conductivity
  • 0.25 - 0.50 mm Thickness

Product Description

Honeywell's TIP3500 thermal insulator pad comes in a blue color and offers thickness ranging from 0.25 - 0.50mm. While the Breakdown voltage between TIP 1500 and TIP 3500 is identical and they are both V0 rated, their dielectric properties differ, mostly as an effect of the different thicknesses. It is ideal for Automotive electronics and Power conversion and supply equipment and comes with a single sided Pressure sensitive adhesive for easy assembly.

Honeywell's TIP3500 thermal insulator pad is designed to provide low thermal impedance and high isolation for high power and high voltage applications. Integrated fiberglass reinforcement protects the pad from tears, cut-throughs and punctures.It is designed to be soft and conformal which provides excellent mating surface for low pressure mounting. Please consult the Specification fields and the Technical data sheets for additional information

Product Family

SOLSTICE TIP3500

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
EU Shipping in 8 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Blue
Film Thickness
0.25 - 0.50 mm
Specific Gravity
2.47
Thermal Properties
Thermal Conductivity
3.5 W/m.K
Thermal Impedance
0.18 - 0.23 °C·cm²/W
UL 94 Rating
V-0
Electrical Properties
Breakdown Voltage
>6000 V
Volume Resistivity
50000000000000 Ohms⋅cm

Leading Brands Trust in Our Products and Services