PTM 7900 | Phase Change Pad

Harmonization Code : 8473.30.80.00 | Parts and accessories (other than covers, carrying cases and the like) suitable for use solely or principally with machines of headings 8470 to 8472 ; Parts and accessories of the machines of heading 8471 ; Other; Other

PTM7900| Phase Change Pad PTM7900| Phase Change Pad

Main features

  • 0.045 Thermal Impedance
  • 8.0 Thermal Conductivity
  • Pad form

Product Description

PTM7900 is designed to minimize thermal resistance at interfaces and maintain extremely stable performance through reliability testing required for long product life applications. It has stable Thermal Impedance across accelerated aging tests and does not display bleed, pump or flow out. PTM7XXX product line has the highest Thermal conductivity and lowest thermal impedance out of the entire PTM Series

PTM7900 has a Thermal conductivity of 8.0 (W/m·K) depending on the bondline thickness and is based on a robust polymer PCM structure that exhibits excellent wetting properties during typical operating temperature ranges, resulting in very low surface contact resistance. This proprietary material provides superior reliability and maintains low thermal impedance (0.045) , making it desirable for high-performance integrated circuit devices. It has been qualified from major GPU and cooling solution manufacturers across the globe.

PTM7900 is almost as good as it gets. The only product that has slightly better thermal properties is PTM7950 which reaches 8.5 W/m·K and 0.04 TI and is designed for extremely demanding and tight applications.

PTM7900 and PTM7950 are closely related thermal interface materials with slight differences in performance. PTM7950 features a softer composition, higher thermal conductivity, and lower thermal impedance, enhancing its overall thermal performance. Aside from these improvements, both materials share similar characteristics.

Product Family

SOLSTICE PTM7900

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
EU Shipping in 8 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific Gravity
2.8
Thickness range
0.20 - 1.00 mm
Thermal Properties
Specific Heat Capacity
0.97 J/(g⋅°C)
Thermal Conductivity
8.0 W/m.K
Thermal Impedance
0.046 °C·cm²/W
Electrical Properties
Volume Resistivity
210000000000000 Ohms⋅cm

Additional Information

What are the reliability expectations of the PTM 7XXX products?


All the 7XXXseries (7000, 7900 & 7950) pass the three major reliability tests with flying colours. Honeywell does not test beyond 1000 cycles, 92 hrs HAST and 1000 hrs HTS. However, anecdotally, some automotive customers have taken 7900 to beyond Honeywell’s limits and have found it to pass shock and vibration, longer temperature cycling and longer temperature and humidity soak.
If your lifetime performance is defined mainly by power cycling, then you also check the 6000 series which will have the longest life.
 
The main difference between the 7XXX products is the filler content which makes 7950 the most conductive.
 

PTM7XXX Series vs Competition comparison

 

PTM 7900 Bondline Thickness vs Pressure Curve

PTM 7900 BLT vs Pressure Curve

Leading Brands Trust in Our Products and Services