HT 4500 | One part Hybrid Thermal Gel

Harmonization Code : 3824.99.96.99 | Prepared binders for foundry moulds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included : Other : Other: Other

HT4500 | One part Hybrid Gap Filler

Main features

  • Green
  • 4.5 Thermal Conductivity
  • Printable

Product Description

Honeywell HT4500 is a pre cured dispensable/printable gap filler which is silicone-based and filled with advanced ceramic fillers. It is formulated to deliver high dispense rate for improved productivity, good gap filling ability under low pressure and low contamination to devices. The viscosity is modified and developed specifically to allow it to be integrated into printing processes. The material is designed to minimise thermal resistance at interfaces and maintain excellent performance through reliability testing.

Honeywell HT4500 is designed for those that prefer the reliability of a gel material for their printing processes. The low viscosity that enables printing removes the need for expensive dispensing equipment and makes for a good alternative for thermal greases that often exhibit pump out or dry out issues. As an additional bonus, HT4500 has been extensively tested and passed the rigorous vibration tests that are required by the automotive industry. HT4500 has excellent thermal stability after different long term reliability tests including, D85( 85 ̊C&85%RH) 1000hrs, Thermal Shock 1000cycles and HTB(High Temperature Baking)150 ̊C 1000hrs.

Honeywell HT4500 is a soft, printable gel that can be applied like grease using screen printing. There is almost no stress when being compressed and compression-deflection is difficult to measure. Slumping is a concern when bondline thickness is high; especially if the boards are vertically mounted. For HT4500, we recommend less than 1mm( in vertical position) to prevent slumping but thickness is not a concern at all when boards are horizontally mounted.

Product Family

SOLSTICE HT4500

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
EU Shipping in 8 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Green
Specific Gravity
3.3
Thermal Properties
Thermal Conductivity
4.5 W/m.K
Electrical Properties
Dielectric Strength
5 kV/mm
Volume Resistivity
10000000000000 Ohms⋅cm

Additional Information

Minimum BLT for HT 4500 is around 0.15mm. Maximum BLT is a function of the size of the components being attached and pressure. A reasonable value could be 1mm