HLT 3500LV | Two part Hybrid Thermal Gel

Harmonization Code : 3824.99.96.99 | Prepared binders for foundry moulds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included : Other : Other: Other

HLT 3500LV | Two part Hybrid Thermal Gel

Main features

  • Blue + White
  • 3.5 Thermal Conductivity
  • 0.44 Thermal impedance

Product Description

Honeywell HLT3500LV is a two-part, dispensable thermally conductive gel, which offers long-term reliability and superior softness. The enhanced bonding force between the polymer base and the filler largely improves the thermally conductive gel oil separation issue in storage. Prior to curing, the material maintains good thixotropic characteristics and low viscosity to be easily dispensed. The product can be cured in short time after two- component mixing at room temperature. The high compressibility minimizes thermal resistance at interfaces, while maintaining excellent performance during reliability testing. It is the Low Volatiles version of HLT 3500 with less than 50ppm on Σ D3-D20.

Honeywell HLT3500LV is a balanced solution for Vertical mounting that requires high TC before we go into the upper end of the product line. The enhanced bonding force between the polymer base and the filler largely improves the thermally conductive gel oil separation issue in storage.  Prior to curing, the material maintains good thixotropic characteristics and low viscosity to be easily dispensed.

Cure Schedule

  • 18 hours at Room temperature or
  • 30minutes at 100°C.

These are just indications. You can experiment with curing for your application needs.

Product Family

SOLSTICE HLT3500LV

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
EU Shipping in 8 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
White and Red
Specific Gravity
3.1
Thermal Properties
Thermal Conductivity
3.5 W/m.K
Thermal Impedance
0.44 °C·cm²/W
Physical Properties
Viscosity
200,000 - 400,000 mPa.s

Leading Brands Trust in Our Products and Services