HLT 2000LV | Two part Hybrid Thermal Gel

Harmonization Code : 3824.99.96.99 | Prepared binders for foundry moulds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included : Other : Other: Other

HLT 2000LV | Two part Hybrid Thermal Gel

Main features

  • White + Dark Red
  • 2.0 Thermal Conductivity
  • Low volatility

Product Description

Honeywell HLT 2000LV is a two-part, dispensable thermally conductive gel, which offers long-term reliability and superior softness. Its properties are identical to HLT2000 and the main differences are the slightly lower Thermal impedance (0.60), lower volatility and longer Cure time at room temperature. The enhanced bonding force between the polymer base and the filler largely improves the thermally conductive gel oil separation issue in storage.  Prior to curing, the material maintains good thixotropic characteristics and low viscosity to be easily dispensed.

Honeywell HLT 2000LV can be cured in short time after two-component mixing at room temperature. The high compressibility minimizes thermal resistance at interfaces, while maintaining excellent performance during reliability testing.

The product can be cured at either 16 hours at Room temperature or 30minutes at 100°C. Of course those are just indications and you can experiment with curing for your application needs.

Product Family

SOLSTICE HLT2000LV

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
EU Shipping in 8 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
White - Dark Red
Specific Gravity
2.8
Thermal Properties
Thermal Conductivity
2.0 W/m.K
Thermal Impedance
0.60 °C·cm²/W
Physical Properties
Viscosity
200,000 - 400,000 mPa.s