SILASTIC RTV-3120

Harmonization Code : 2901.10.00.00 | Acyclic hydrocarbons; Saturated

SILASTIC RTV-3120

Main features

  • 28,000 cP Base Viscosity
  • High-Temperature Mold Service
  • Adjustable Catalyst-Controlled Cure

Product Description

SILASTIC RTV-3120 Mold-Making Base is a red, high-temperature condensation-cure silicone base for producing molds within a documented catalyst and cure system. The base has a typical viscosity of 280 poise (28,000 cP) and a specific gravity of 1.45 at 25 deg C, supporting pourable processing and reproduction of intricate details. A compatible catalyst is selected and added separately; the base alone does not represent the cured mold rubber or its final performance. Use is limited to validated mold geometry, catalyst ratio, release practice, cure schedule, casting material, and service conditions.

Key features

  • 28,000 cP base viscosity: Supports pourable mold preparation at 25 deg C
  • High-temperature mold base: Supports high-temperature mold-making formulations with the documented catalyst
  • Separate catalyst control: Catalyst selection and ratio establish the working and cure profile

Applications

High-temperature silicone mold making within validated mold geometry, catalyst ratio, release practice, cure schedule, and casting conditions.

Product Family

SILASTIC RTV-3120

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Red
Specific Gravity
1.45
Physical Properties
Viscosity
280 mPa.s
Mechanical Properties
Elongation
128 %

Additional Information

Technical properties

As-supplied / before-processing properties

The page entity is the mold-making base only; catalyst selection and cure conditions remain system-dependent.

Property Value Unit Method / condition
Color Red As supplied
Viscosity 280 (28,000) poise (cP) At 25 deg C
Specific gravity 1.45 At 25 deg C
Reference mix ratio 10:1 base:catalyst by weight RTV-3010-S Catalyst reference formulation; catalyst sold separately