SILASTIC 5-8733

Harmonization Code : 2901.10.00.00 | Acyclic hydrocarbons; Saturated

SILASTIC 5-8733

Main features

  • Fuel-Resistant Fluorosilicone Chemistry
  • One-Part Cartridge Application
  • 190% Cured Elongation

Product Description

DOWSIL 5-8733 Fluorosilicone Sealant is a gray, one-part moisture-curing sealant for bonding, sealing, and caulking where resistance to documented fuels, solvents, and chemicals is required. The ready-to-use paste is supplied in a 225 g cartridge and has a typical specific gravity of 1.4. After cure, typical commercial properties include 46 Shore A hardness, 400 psi tensile strength, and 190% elongation. Its fluorosilicone chemistry supports aerospace, automotive, and industrial sealing evaluations involving jet fuel, gasoline, or solvent exposure, provided the exact substrate, fluid, concentration, temperature, duration, cure, and joint configuration are validated.

Key features

  • One-part cartridge application: Ready-to-use gray paste in a 225 g package
  • Fuel and solvent resistance: Supports sealing evaluations under documented chemical-exposure conditions
  • 190% cured elongation: Typical commercial value for the cured fluorosilicone

Applications

Bonding, sealing, and caulking in aerospace, automotive, and industrial assemblies exposed to validated jet-fuel, gasoline, solvent, or chemical conditions.

Product Family

SILASTIC 5-8733

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Gray
Specific Gravity
1.4
Physical Properties
Tack-Free Time
30 minutes
Mechanical Properties
Elongation
190 %
Peel Strength
20 ppi

Additional Information

Technical properties

As-supplied / before-processing properties

Property Value Unit Method / condition
Component count 1 part Ready to use
Physical form Paste As supplied
Color Gray As supplied
Specific gravity 1.4 Typical value
Package size 225 g Cartridge
Technical properties

After-processing / final-state properties

Typical values; test methods are not stated in the authorized commercial product detail.

Property Value Unit Method / condition
Hardness 46 Shore A Typical commercial value; method not stated
Tensile strength 400 psi Typical commercial value; method not stated
Elongation 190 % Typical commercial value; method not stated