SILASTIC 3112

Harmonization Code : 2901.10.00.00 | Acyclic hydrocarbons; Saturated

SILASTIC 3112

Main features

  • 28,000 cP Base Viscosity
  • Adjustable Catalyst-Controlled Cure
  • Simple-Pattern Mold Making

Product Description

SILASTIC RTV-3112 Mold-Making Base is a white, general-purpose condensation-cure silicone base for producing simple molds without deep undercuts. The base has a typical viscosity of 280 poise (28,000 cP) and a specific gravity of 1.30 at 25 deg C, supporting pourable processing and reproduction of detailed patterns. A compatible catalyst is selected and added separately to establish the working and cure profile; the base is not a complete mold-making system by itself. Use is limited to mold geometries, catalyst ratios, release practices, and cure conditions validated for the intended pattern and casting material.

Key features

  • 28,000 cP base viscosity: Supports pourable mold preparation at 25 deg C
  • Separate catalyst control: Catalyst selection and ratio establish the working and cure profile
  • Detailed pattern reproduction: Low mixed viscosity supports replication of intricate features

Applications

General-purpose silicone mold making for simple patterns without deep undercuts, using a compatible catalyst and validated release and cure process.

Product Family

SILASTIC 3112

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
White
Specific Gravity
1.30
Physical Properties
Viscosity
280 mPa.s
Mechanical Properties
Elongation
127 %

Additional Information

Technical properties

As-supplied / before-processing properties

The page entity is the mold-making base only; catalyst selection and cure conditions remain system-dependent.

Property Value Unit Method / condition
Color White As supplied
Viscosity 280 (28,000) poise (cP) At 25 deg C
Specific gravity 1.30 At 25 deg C
Reference mix ratio 10:1 base:catalyst by weight RTV-3010-S Catalyst reference formulation; catalyst sold separately