SIKA SIKALASTOMER- 511 NON-SKINNING BUTYL SEALANT

Harmonization Code : 8547.90.00.00 | Insulating fittings for electrical machines, appliances or equipment, being fittings wholly of insulating material apart from any minor components of metal (for example, threaded sockets) incorporated during moulding solely for purposes of assembly, other than insulators of heading 8546; electrical conduit tubing and joints therefor, of base metal

SIKA SIKALASTOMER- 511 NON-SKINNING BUTYL SEALANT

Main features

  • Non-Corrosive Sealing Formulation
  • Standing-Seam Roof and Wall-Panel Sealing
  • 50 to 105 deg C Service Range

Product Description

SikaLastomer®-511 is a one-part, non-skinning and non-corrosive butyl-rubber sealant for factory sealing standing-seam roof and wall panels and concealed end laps. The off-white material remains malleable after application, allowing metal panels to be separated later for repair or maintenance. It is applied to clean surfaces using manual, pneumatic, electric, or pump equipment within a documented application-temperature range of 5°C to 40°C. The sealant has a typical uncured density of 1.09 kg/L and a service-temperature range of -50°C to 105°C.

Key features

  • Non-skinning butyl sealant: The material remains malleable after application and supports later panel separation.
  • Factory-to-field assembly window: Panels may be joined in the field up to six months after initial application under the documented conditions.
  • Wide service range: The documented service-temperature range is -50°C to 105°C.

Applications / Suitable for

  • Factory sealing of standing-seam roof panels
  • Standing-seam wall panels
  • Concealed panel end laps
Product Family

SIKALASTOMER 511

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Off-white
Density (g)
1.09 g/cm3
Thermal Properties
Service temperature
-50 ─ 105 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or mixed-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Chemical base Butyl N/A As supplied
Color Off-white N/A CQP001-1
Uncured density 1.09 kg/L Typical product data
Application temperature 5 to 40 °C Ambient
Slump 1 mm ASTM D2202 at 23°C and 50% RH
Shelf life 12 months Cartridges, pails, or drums stored below 25°C
Technical properties

After-processing / final-state properties

Typical final-state values under the stated system and test conditions. These values are not sales specifications.

Property Value Unit Method / condition
Service temperature -50 to 105 °C Documented range
Shrinkage 16 % CQP014-1
Heat-aging weight loss 11 % ASTM C792
Staining No staining N/A ASTM D925 on common substrates