Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

SIKAFLEX 255FC

Main features

  • Fast-Curing Direct Glazing
  • 20-Minute Glazing Open Time
  • Non-Sag Glazing Bead Application

Product Description

Sikaflex-255 FC is a fast-curing, one-component polyurethane adhesive for direct glazing and glass replacement in commercial vehicles. The black material has very good non-sag properties, a 20-minute open time, and a 40-minute skin time at 23 deg C and 50% relative humidity, supporting controlled glass installation in warm conditions. After cure, typical properties include 6 MPa tensile strength, 450% elongation, 12 N/mm tear propagation resistance, and 4 MPa tensile lap-shear strength. The adhesive is compatible with Sika's black-primerless bonding process for mineral-glass windows within the prescribed pretreatment system.

Key features

  • Fast-curing glazing: The adhesive is formulated for commercial-vehicle direct glazing and glass replacement
  • 20-minute open time: Defines the glass-installation window at 23 deg C and 50% relative humidity
  • Non-sag bead control: Very good non-sag properties support triangular-bead application

Applications

Commercial-vehicle direct glazing; mineral-glass window installation; vehicle glass replacement; Sika black-primerless bonding processes.

Product Family

SIKAFLEX 255FC

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
polyurethane
Color
black
Component System
one
Density
1.2 kg/m3
Mechanical Properties
Elongation
450 %
Thermal Properties
Operating Temperature
-40 to 90 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Property Value Unit Method / condition
Chemical base 1-component polyurethane As supplied
Color Black CQP001-1
Density 1.2 kg/l Uncured
Non-sag properties Very good As supplied
Application temperature 10 to 35 deg C Product and ambient range
Skin time 40 minutes CQP019-1; 23 deg C / 50% RH
Open time 20 minutes CQP526-1; 23 deg C / 50% RH
Shelf life - cartridge / unipack 9 months Storage below 25 deg C
Technical properties

After-processing / final-state properties

Property Value Unit Method / condition
Shrinkage 3 % CQP014-1
Hardness 60 Shore A CQP023-1 / ISO 48-4
Tensile strength 6 MPa CQP036-1 / ISO 527
Elongation at break 450 % CQP036-1 / ISO 527
Tear propagation resistance 12 N/mm CQP045-1 / ISO 34
Tensile lap-shear strength 4 MPa CQP046-1 / ISO 4587