SIKAFLEX 201

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

SIKAFLEX 201

Main features

  • Long Four-Hour Skin Time
  • Non-Sag Industrial Joint Sealing
  • Sandable and Paintable Surface

Product Description

Sikaflex-201 US is a one-component, moisture-curing polyurethane sealant for permanent flexible and elastic industrial seals. Its non-sag consistency supports controlled joint filling, while a four-hour skin time at 23 deg C and 50% relative humidity allows additional working time before tooling. The cured sealant has 550% elongation and a Shore A hardness of 45 under ASTM D412 and CQP023-1 / ISO 48-4. It can be sanded and painted after skin formation and is used for joints, seams, and gaps in HVAC systems, metal buildings, tanks, grain bins, and non-vehicular window perimeters.

Key features

  • Long tooling window: Four-hour skin time allows additional working time at 23 deg C and 50% relative humidity
  • Non-sag application: Good non-sag properties support controlled joint filling
  • Elastic cured seal: ASTM D412 elongation at break is 550%

Applications

Sealing joints, seams, and gaps in HVAC systems, metal buildings, tanks, grain bins, and non-vehicular window perimeters.

Product Family

SIKAFLEX 201

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
polyurethane
Component System
one
Density
1.5 kg/m3
Mechanical Properties
Elongation
550 %
Thermal Properties
Operating Temperature
-40 to 90 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Property Value Unit Method / condition
Chemical base 1-component polyurethane As supplied
Color White, aluminum gray, tan, capitol tan, MB bronze, black CQP001-1
Density 1.5 kg/l Uncured
Non-sag properties Good As supplied
Application temperature 5 to 40 deg C Product and ambient range
Skin time 4 hours CQP019-1; 23 deg C / 50% RH
Shelf life - cartridge / unipack 12 months Storage below 25 deg C
Shelf life - pail / drum 6 months Storage below 25 deg C
Technical properties

After-processing / final-state properties

Property Value Unit Method / condition
Hardness 45 Shore A CQP023-1 / ISO 48-4
Tensile strength 1.3 MPa ASTM D412
Elongation at break 550 % ASTM D412
Service temperature -40 to 90 deg C CQP513-1