SIKAFAST 321S

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

SIKAFAST 321S

Main features

  • Fast Five-Minute Open Time
  • Built-In Bondline Spacing
  • Stanchion and Assembly Bonding

Product Description

SikaFast-321 S is a shimmed, two-component methacrylate structural adhesive for stanchion and general assembly bonding. Incorporated 0.68 to 0.84 mm spacers maintain a uniform bond thickness, while the 10:1 volume-mix thixotropic paste provides a five-minute open time at 23 deg C. The cured material reaches 80% elongation and a typical tensile lap-shear strength of 10.5 MPa under ASTM D638 and CQP046-6 / ISO 4587. It is suited to concealed-joint fastening on aluminum, stainless steel, galvanized steel, and fiber-reinforced polymers, including assemblies where adhesive bonding replaces or complements rivets, screws, or welding.

Key features

  • Controlled bond thickness: Incorporated 0.68 to 0.84 mm spacers maintain a uniform bondline
  • Five-minute open time: Supports rapid assembly at 23 deg C and 50% relative humidity
  • Ductile structural profile: Typical cured elongation is 80% with 10.5 MPa tensile lap-shear strength

Applications

Stanchion and general assembly bonding; high-strength fastening of concealed joints; bonding aluminum, stainless steel, galvanized steel, and fiber-reinforced polymers.

Product Family

SIKAFAST 321S

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Methacrylate
Color
Dark Gray, Straw
Density (g)
0.99 g/cm3
Mechanical Properties
Elongation
80 %

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for SikaFast-321 S Part A, SikaFast-3081 N Part B, and the mixed adhesive system.

Property Value Unit Method / condition
Part A density 0.96 kg/l SikaFast-321 S Part A
Part B density 1.30 kg/l SikaFast-3081 N Part B
Mixed density 0.99 kg/l Calculated mixed value
Mix ratio by volume 10:1 Part A:Part B
Consistency Thixotropic paste Mixed adhesive
Spacer shim thickness 0.68 to 0.84 mm Incorporated spacers
Application temperature 10 to 35 deg C Substrate and adhesive range
Open time 5 minutes CQP526-2; 23 deg C / 50% RH
Technical properties

After-processing / final-state properties

Typical cured values for the mixed adhesive system.

Property Value Unit Method / condition
Hardness 65 Shore D CQP023-1 / ISO 48-4
Tensile strength 9 MPa ASTM D638
Elongation at break 80 % ASTM D638
E-modulus at 0-5% elongation 100 MPa ASTM D638
Tensile lap-shear strength 10.5 MPa CQP046-6 / ISO 4587