SIKABIRESIN CF234

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

SIKABIRESIN CF234

Main features

  • 24-part hardener weight ratio
  • 0.43 g/cm3 Part B density
  • Honeycomb edge-fill system hardener

Product Description

SikaBiresin CF234 Part B Hardener is the green amine paste component for the two-part CF230/CF234 epoxy edge-filling system. It is mixed with CF230 Part A at 24 parts hardener to 100 parts resin by weight. Part B has a typical specific gravity of 0.43 at 25 deg C; the combined material has a typical 11-minute pot life at the same temperature. The system forms a lightweight, smooth paste for honeycomb edge filling, cell densification around inserts, and localized sandwich-panel repairs. Final mechanical, thermal, flame-test, shrinkage, and machinability data apply only after CF234 is combined and cured with the specified CF230 Part A resin.

Key features

  • Controlled hardener ratio: Use 24 parts CF234 to 100 parts CF230 by weight
  • Low-density Part B: The green amine paste has a typical specific gravity of 0.43 at 25 deg C
  • Short mixed pot life: The 116 g CF230/CF234 mixture has an 11-minute pot life at 25 deg C

Applications

Edge filling of aluminum and other honeycomb sandwich structures; core-cell densification for insert anchoring; localized sandwich-panel repairs.

Product Family

SIKABIRESIN CF234

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
paste
Chemistry Type
amine
Color
green
Component System
two
Specific Gravity
0.43

Additional Information

Technical properties

As-supplied / before-processing properties

Part B properties are separated from processing values for the complete CF230/CF234 system.

Property Value Unit Method / condition
Composition Amine CF234 Part B
Aspect Paste As supplied
Color Green CF234 Part B
Specific gravity 0.43 g/cm3 At 25 deg C
System mix ratio by weight 100:24 CF230 Part A:CF234 Part B
Mixed-system pot life 11 minutes 116 g mixture at 25 deg C
Shelf life 12 months Original unopened container at 15-25 deg C