RTVS 3-95-2

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

RTVS 3-95-2

Main features

  • 1:1 weight or volume mix
  • 1.44 W/(m K) thermal conductivity
  • -55 to 260 deg C service range

Product Description

INSULCAST RTVS 3-95-2 Thermally Conductive Silicone Potting Compound is a two-part, 1:1 red-and-white RTV silicone system for thermally conductive electrical potting and encapsulation. Parts A and B each have a typical viscosity of 35,000 cP at 25 deg C, and the mixed material provides a 1.5-hour pot life at the same temperature. Room-temperature and accelerated heat-cure schedules support different production windows. After cure, the silicone combines 1.44 W/(m K) thermal conductivity with electrical insulation, 85 Shore A hardness, and a service range from -55 to 260 deg C. Applications include protected electronic assemblies requiring heat transfer and dielectric performance.

Key features

  • Simple 1:1 mixing: Parts A and B use the same ratio by weight or volume
  • Flexible cure scheduling: Room-temperature and accelerated heat-cure options are available
  • Thermal and electrical function: Cured material combines 1.44 W/(m K) conductivity with dielectric properties

Applications

Potting and encapsulation of electronic assemblies requiring thermal conductivity, electrical insulation, and high-temperature service.

Product Family

RTVS 3-95-2

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Component System
Two Part
Mechanical Properties
Elongation
17 %
Thermal Properties
Service temperature
-55 to 260 °C
Thermal Conductivity
1.44 W/m.K
UL 94 Rating
V0

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uncured values; maintain the stated component identity and 1:1 ratio.

Property Value Unit Method / condition
Part A color Red As supplied
Part B color White As supplied
Component viscosity 35,000 cP ASTM D2393 at 25 deg C; Parts A and B
Specific gravity 2.36 / 2.27 Part A / Part B at 25 deg C
Mix ratio 1:1 By weight or volume
Mixed viscosity 35,000 cP At 25 deg C
Pot life 1.5 hours At 25 deg C
Gel time 2-4 hours At 25 deg C
Technical properties

After-processing / final-state properties

Typical cured properties; final performance depends on the selected cure schedule and test condition.

Property Value Unit Method / condition
Thermal conductivity 1.44 W/(m K) ASTM D5470
Hardness 85 Shore A Cured material
Tensile strength 400 psi ASTM D412; 2.9 MPa
Elongation 17 % ASTM D412
Dielectric strength 425 V/mil Cured material
Volume resistivity 1 x 10^14 / 1 x 10^13 ohm-cm At 25 deg C / 125 deg C
Service temperature range -55 to 260 deg C Documented range