ROYAL WS-8072

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

ROYAL WS-8072

Main features

  • Selectable B-1/2 and B-2 work lives
  • Non-sag extrusion and spatula application
  • Corrosion-inhibitive aircraft sealing

Product Description

H.B. Fuller WS-8072 Class B Non-Chromate Corrosion-Inhibitive Sealant is a two-part, manganese-cured polysulfide aircraft sealant supplied in B-1/2 and B-2 work-life grades for corrosion-inhibitive sealing. The lightweight, thixotropic material mixes to a dark brown, non-sag compound that can be applied by extrusion gun or spatula. A 100:7.9 volume ratio or 100:12 weight ratio controls the base-to-curing-agent mix. After cure, the sealant remains flexible at -65 deg F without loss of adhesion or cracking and retains physical properties after limited exposure to aviation fuels and oils. Grade-specific application and assembly times allow selection around the required sealing workflow.

Key features

  • Selectable work-life grades: B-1/2 and B-2 options provide different application and assembly windows
  • Non-sag application: Thixotropic compound supports extrusion-gun or spatula placement
  • Corrosion-inhibitive sealing: Forms a barrier on aluminum and documented dissimilar-metal interfaces

Applications

Aircraft fay-surface and channel sealing; corrosion-inhibitive sealing of aluminum and dissimilar-metal interfaces.

Product Family

ROYAL WS-8072

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Dark brown paste
Chemistry Type
2-part, non-chromate polysulfide corrosion-inhibitive sealant
Specific Gravity
≤1.15

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uncured values for the B-1/2 and B-2 Class B configurations.

Property Value Unit Method / condition
Base color Yellowish Part B
Hardener color Black Part A
Mixed color Dark brown Uncured mixture
Mix ratio by volume 100:7.9 Base:hardener
Mix ratio by weight 100:12 Base:hardener
Uncured viscosity 10,000-15,000 poise Part B base and mixed material
Shelf life 9 months Original unopened container below 80 deg F
Technical properties

After-processing / final-state properties

Typical cured properties; cure development and work-life depend on the selected B-1/2 or B-2 grade.

Property Value Unit Method / condition
Specific gravity 1.15 max Cured material
Nonvolatile content 96 min % Cured material
Hardness 45 Shore A Cured material
Tensile strength >200 psi 14-day standard cure at 77 deg F
Elongation >250 % MIL-PRF-81733 test basis
Continuous service temperature -54 to 250 deg F Operating range
Intermittent temperature excursion Up to 360 deg F Short-duration exposure