ROYAL WS-8070

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

ROYAL WS-8070

Main features

  • Corrosion-inhibitive aerospace sealing
  • Non-sag extrusion handling
  • Two Class B work lives

Product Description

Royal Sealants WS-8070 Class B Corrosion-Inhibitive Aerospace Sealant is a two-part, manganese-cured polysulfide paste for corrosion-inhibitive sealing of aircraft structures. The non-sag Class B material is applied by extrusion gun or spatula to fillet and faying surfaces where water intrusion and dissimilar-metal interaction can contribute to corrosion. B-1/2 and B-2 variants provide 0.5- and 2-hour application lives with separate tack-free and cure schedules. After cure, the gray sealant provides documented tensile, elongation, low-temperature-flexibility, and thermal-stability properties under the cited aerospace test conditions.

Key features

  • Corrosion-inhibitive sealing: Targets water intrusion and dissimilar-metal interfaces
  • Non-sag thixotropic paste: Applies by extrusion gun or spatula
  • Two Class B profiles: Provides 0.5- or 2-hour application life

Applications

Fillet and faying-surface sealing of aircraft structures where the documented WS-8070 Class B process and corrosion-inhibitive scope apply.

Product Family

ROYAL WS-8070

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Gray when mixed
Chemistry Type
2-part, manganese-cured polysulfide corrosion-inhibitive sealant
Specific Gravity
1.46

Additional Information

Technical properties

As supplied / before processing

Property Value Unit Method / condition
Product form Thixotropic non-sag paste - Typical at 77 deg F and 50% RH
Base viscosity 8,000 to 12,000 poise Brookfield No. 7 spindle at 2 rpm; 77 deg F and 50% RH
Component and mixed color Part A black; Part B yellow; mixed gray - Before and after mixing
Mix ratio by weight 100:10 - Base:accelerator
Mix ratio by volume 100:8.39 - Base:accelerator
Application life 0.5 / 2 h Class B-1/2 / Class B-2; 77 deg F and 50% RH
Tack-free time 5 to 6 / 6 to 7 h Class B-1/2 / Class B-2; 77 deg F and 50% RH
Technical properties

After processing / final state

Property Value Unit Method / condition
Tensile strength 430 psi Typical after 14 days at 75 deg F and 50% RH; MIL-PRF-81733
Ultimate elongation 330 % Typical after 14 days at 75 deg F and 50% RH; MIL-PRF-81733
Final hardness 48 Shore A Cured material
Specific gravity 1.46 - Cured material
Nonvolatile content 95 % Cured material
Low-temperature flexibility No cracking, checking, or adhesion loss - At -65 deg F
Thermal stability No blistering, cracking, or hardness deviation - After 48 h at 320 deg F