ROYAL WS-8035

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

ROYAL WS-8035

Main features

  • Rapid-cure Class B profile
  • Lightweight cured specific gravity
  • Documented electrical resistivity

Product Description

Royal Sealants WS-8035 Class B Rapid-Cure Lightweight Aerospace Sealant is a two-part rapid-cure lightweight polysulfide sealant for aerospace and space-exploration fuel tank or fuselage assemblies. The Class B system uses controlled base-to-accelerator ratios and provides a B-2 application life of about two hours. Its mixed viscosity supports sealant application before room-temperature cure, while the cured material combines low specific gravity with defined tensile strength, elongation, Shore A hardness, and electrical resistivity. Documented final-state data also include intermittent temperature exposure up to 360 deg F.

Key features

  • Rapid-cure Class B system: Provides an approximately two-hour B-2 application life
  • Lightweight cured sealant: Limits cured specific gravity to 1.1
  • Defined electrical behavior: Provides documented cured volume resistivity

Applications

Aerospace and space-exploration fuel tank or fuselage sealing where the documented WS-8035 Class B process and qualification scope apply.

Product Family

ROYAL WS-8035

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Dark gray paste
Chemistry Type
2-part, lightweight rapid-cure polysulfide fuel-tank sealant
Specific Gravity
≤1.10

Additional Information

Technical properties

As supplied / before processing

Property Value Unit Method / condition
Product format Two-component polysulfide sealant - Base and accelerator system
Mix ratio by volume 100:7.06 - Base:accelerator
Mix ratio by weight 100:12 - Base:accelerator
Mixed viscosity Approx. 3,900 cP Mixed material
Application life Approx. 2 h Class B-2
Tack-free time Less than 7 h Class B-2
Shelf life 9 months Documented storage life
Technical properties

After processing / final state

Property Value Unit Method / condition
Cured specific gravity Max. 1.1 - Cured material
Tensile strength Approx. 258 psi Cured material
Ultimate elongation Approx. 250 % Cured material
Final hardness Approx. 45 Shore A Cured material
Volume resistivity Approx. 6 x 10^9 ohm m Cured material
Intermittent exposure Up to 360 deg F Documented intermittent condition