Royal Sealants WS-8032 Class B Ultra-Lightweight Fast-Cure Fuel Tank and Fuselage Sealant is a two-part, manganese-dioxide-cured polysulfide paste for aircraft fuel tank and fuselage sealing. The Class B material combines an ultra-lightweight formulation with fast room-temperature cure and low-sag, thixotropic handling. It can be applied by extrusion gun or spatula and is documented for sealing service from -65 to 250 deg F, with intermittent exposure up to 360 deg F. The B-2 configuration provides a defined Class B process option for applications requiring its associated work-life and cure schedule.

Key features

  • Ultra-lightweight formulation: Uses a reduced-density formulation for weight-sensitive sealing
  • Fast-cure Class B system: Supports shorter room-temperature processing
  • Low-sag paste: Applies by extrusion gun or spatula
Product Family

ROYAL WS-8032

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Dark gray paste
Chemistry Type
1-part, water-based natural rubber contact adhesive
Specific Gravity
1.10

Additional Information

Technical properties

As supplied / before processing

Property Value Unit Method / condition
Documented variant Class B-2 - Documented Class B configuration
Product form Low-sag thixotropic paste - Uncured material
Component count Two - Base and accelerator system
Cure system Manganese-dioxide-cured polysulfide - Room-temperature cure
Application method Extrusion gun or spatula - Documented handling method
Technical properties

After processing / final state

Property Value Unit Method / condition
Service temperature -65 to 250 deg F Documented sealing range
Intermittent exposure Up to 360 deg F Documented intermittent condition
Fluid-exposure behavior Retains elastomeric properties - After prolonged exposure to jet fuel and aviation gasoline