ROYAL WS-8020RC

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

ROYAL WS-8020RC

Main features

  • Rapid room-temperature cure
  • Low-sag thixotropic application
  • Fuel and oil resistance

Product Description

Royal Sealants WS-8020RC Class B Rapid-Cure Fuel Tank and Fuselage Sealant is a two-part rapid-cure polysulfide paste for aircraft fuel tank and fuselage sealing. The low-sag, thixotropic material applies by extrusion or spatula spreading and cures at room temperature. Its documented property set includes fuel and oil resistance, low-temperature flexibility at -65 deg F, and an intermittent exposure limit of 360 deg F. The Class B system is supplied as base and accelerator components and uses controlled mix ratios by weight or volume for consistent preparation before application.

Key features

  • Rapid room-temperature cure: Supports shortened sealant processing cycles
  • Low-sag thixotropy: Controls placement during extrusion or spatula application
  • Fuel and oil resistance: Supports documented aerospace fluid-exposure conditions

Applications

Aircraft fuel tank and fuselage sealing where the documented rapid-cure Class B polysulfide process and fuel or aviation-fluid exposure scope apply.

Product Family

ROYAL WS-8020RC

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Dark gray paste
Chemistry Type
2-part, rapid-cure polysulfide fuel-tank / aerospace sealant
Specific Gravity
≤1.45

Additional Information

Technical properties

As supplied / before processing

Property Value Unit Method / condition
Product form Paste - As supplied
Product format Two-component sealant - Base and accelerator system
Chemical family Polysulfide - Reactive sealant chemistry
Application method Extrusion or spatula spreading - Apply after substrate preparation
Mix ratio by volume 100:10.14 - By volume
Mix ratio by weight 100:12 - By weight
Technical properties

After processing / final state

Property Value Unit Method / condition
Low-temperature flexibility No loss of adhesion or cracking - At -65 deg F
Intermittent exposure temperature Max. 360 deg F Documented intermittent exposure
Nonvolatile content Min. 97 % Cured material
Specific gravity Max. 1.45 - Cured material
Fuel swell Max. 6.5 % AMS 2629, test method Type 1
Tensile strength Min. 350 psi At 77 deg F after 14-day standard cure
Ultimate elongation Min. 300 % At 77 deg F after 14-day standard cure
Ultimate hardness 52 Shore A Cured material