ROYAL WS-8010

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

ROYAL WS-8010

Main features

  • Low-adhesion removable gasket
  • Two Class B work lives
  • Low-sag room-temperature cure

Product Description

Royal Sealants WS-8010 Class B Access Door Sealant is a two-part, manganese-dioxide-cured polysulfide paste that forms a low-adhesion gasket for aircraft access doors and related removable panels. The thixotropic, low-sag material can be applied by extrusion gun or spatula and cures at room temperature. Class B-1/2 and B-2 variants provide application lives of 0.5 and 2 hours, respectively, with separate tack-free and cure schedules. The cured red sealant is formulated for service from -65 to 250 deg F while retaining the low-adhesion behavior required for later panel removal.

Key features

  • Low-adhesion gasket: Supports sealing of removable access doors and panels
  • Two Class B profiles: Provides 0.5- or 2-hour application life
  • Low-sag paste: Applies by extrusion gun or spatula

Applications

Sealing aircraft access doors and related removable panels where a low-adhesion, room-temperature-cured Class B polysulfide gasket is specified.

Product Family

ROYAL WS-8010

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Red paste
Chemistry Type
2-part polysulfide access-door sealant
Specific Gravity
1.45

Additional Information

Technical properties

As supplied / before processing

Property Value Unit Method / condition
Product form Thixotropic low-sag paste - Typical at 77 deg F and 50% RH
Component and mixed color Part A black; Part B red; mixed red - Before and after mixing
Base viscosity 8,000 to 10,000 poise Brookfield No. 7 spindle at 2 rpm; 77 deg F and 50% RH
Slump Less than 0.2 in Class B-1/2 and B-2; 77 deg F and 50% RH
Mix ratio by weight 100:10 - Base:accelerator
Mix ratio by volume 100:8.3 - Base:accelerator
Application life 0.5 / 2 h Class B-1/2 / Class B-2; 77 deg F and 50% RH
Technical properties

After processing / final state

Property Value Unit Method / condition
Specific gravity 1.45 - Typical after 14 days at 77 deg F and 50% RH; AMS-3284
Final hardness 55 Shore A Typical after 14 days at 77 deg F and 50% RH; AMS-3284
Nonvolatile content 98 % Typical cured material
Low-temperature flexibility No cracking or adhesion loss - At -65 deg F
Hydrocarbon weight loss Less than 6 % AMS 2629 JRF; 7 days at 140 deg F
Hydrocarbon swell 6.5 % AMS 2629 JRF; 7 days at 140 deg F