ROYAL RP-5

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

ROYAL RP-5

Main features

  • Fast-setting general-purpose adhesive with 5-second fixture
  • Low 5 cps viscosity
  • Grit-blasted steel shear strength of 28 N/mm²

Product Description

RP5 General Purpose Adhesive is a medium-setting adhesive designed to bond a wide variety of similar and dissimilar materials. The clear, low-viscosity material has a reported viscosity of 5 cps and develops handling strength in 5 to 10 seconds, with full cure in 8 hours. The product is described as providing climatic, thermal, and impact resistance, while its elasticity supports bonding between dissimilar materials. Documented strength testing includes steel, aluminum, ABS, PVC, polycarbonate, phenolic, neoprene rubber, and nitrile rubber substrates.

Key features

  • Fast fixture and handling: Fixture cure is reported at 5 seconds, with handling strength developing in approximately 5 to 10 seconds.
  • Low-viscosity formulation: 5 cps viscosity supports application where a low-viscosity adhesive is required.
  • Broad documented substrate testing: Strength data are provided for metals, engineering plastics, phenolic, and rubber substrates.

Applications / Suitable for

  • General-purpose bonding of similar or dissimilar materials
  • Bonding applications involving metals, plastics, phenolic, and rubber substrates represented in the documented test data
Product Family

ROYAL RP-5

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Clear
Specific Gravity
1.05
Physical Properties
Viscosity
5 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Selected physical and processing properties of RP5 before full cure.

Property Value Unit Method / condition
Color Clear - As supplied
Base Ethyl - Source terminology
Viscosity 5 cps Physical property
Specific gravity 1.05 - Physical property
Fixture cure 5 seconds Reported cure speed for fixture
Handling strength 5 to 10 seconds Reported handling-strength development
Full cure 8 hours Reported full-cure time
Technical properties

After-processing / final-state properties

Selected cured adhesive strength and temperature data for RP5 under the stated substrate and test configurations.

Property Value Unit Method / condition
Shear strength 28; range 24 to 32 N/mm² Grit-blasted steel; ASTM D1002 / DIN 53283
Shear strength 20; range 16 to 24 N/mm² Etched aluminum; ASTM D1002 / DIN 53283
Shear strength >7 / >5 / >6 N/mm² ABS / PVC / polycarbonate; ASTM D1002 / DIN 53283; substrate failure noted
Shear strength >12 N/mm² Neoprene rubber and nitrile rubber; ASTM D1002 / DIN 53283; substrate failure noted
Tensile strength 20; range 14 to 28 N/mm² Grit-blasted steel; ASTM D2095 / DIN 53283
Temperature range -65 to 200 °F Reported physical property