PRC-DESOTO PR 870B1/2

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

PRC-DESOTO PR 870B1/2

Main features

  • Class B-1/2 Processing Window
  • Corrosion-Inhibitive Dissimilar-Metal Seal
  • High-Elongation Cured Seal

Product Description

PPG P/S 870 Class B-1/2 Corrosion-Inhibitive Sealant is a two-part, manganese-dioxide-cured polysulfide sealant for corrosion-barrier sealing of aluminum alloys and dissimilar-metal aerospace joints. The Class B-1/2 grade is a low-sag, thixotropic paste applied by extrusion gun or spatula and cured at room temperature. At 25 deg C and 50% RH, it provides a typical 0.5-hour application life, less than 4 hours to tack-free, and 9 hours to 30 Shore A hardness. The cured material has a typical Shore A hardness of 50, 358 psi tensile strength, and 400% elongation. Its service range is -54 to 121 deg C, with intermittent excursions to 135 deg C.

Key features

  • Class B-1/2 processing: A 0.5-hour application life is paired with less than 4 hours to tack-free at 25 deg C and 50% RH.
  • Corrosion-inhibitive joint seal: The polysulfide sealant forms a barrier on aluminum alloys and between dissimilar metals.
  • High-elongation cured seal: Typical cured elongation is 400% with 358 psi tensile strength.

Applications / Suitable for

  • Corrosion-barrier sealing of aluminum aerospace assemblies.
  • Sealing between dissimilar metals in aerospace assemblies.
  • Aerospace joints exposed to fuels and oils.
Product Family

PRC-DESOTO PR 870B1/2

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Component System
Two Part
Specific Gravity
1.48
Thermal Properties
Service temperature
-54 to 121 °C
Mechanical Properties
Elongation
400 %

Additional Information

Technical properties

As supplied / before processing

Values apply to the Class B-1/2 grade unless otherwise stated.

Property Value Unit Method / condition
Part A / Part B colorBlack / White-As supplied
Mixed colorGray-After mixing
Mix ratio by weight17:100-Part A to Part B
Base viscosity11,000 (1,100)Poise (Pa-s)Brookfield #7 at 2 rpm
Application life0.5hClass B-1/2 at 25 deg C, 50% RH
Tack-free time<4hClass B-1/2 at 25 deg C, 50% RH
Cure to 30 Shore A9hClass B-1/2 at 25 deg C, 50% RH
Storage lifeAt least 9monthsBelow 27 deg C in original unopened containers
Technical properties

After processing / final state

Values are typical and apply to the stated cure and test conditions.

Property Value Unit Method / condition
Cured specific gravity1.48-Cured 14 days at 25 deg C, 50% RH
Nonvolatile content95%Typical cured material
Ultimate cure hardness50Shore ACured 14 days at 25 deg C, 50% RH
Tensile strength358 (2,470)psi (kPa)Cured 14 days at 25 deg C, 50% RH
Elongation400%Cured 14 days at 25 deg C, 50% RH
Low-temperature flexibilityNo cracking-At -54 deg C
Service temperature range-54 to 121deg CIntermittent excursions up to 135 deg C