PRC-DESOTO PR 1776M

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

PRC-DESOTO PR 1776M

Main features

  • Low-Density Fuel-Tank Sealing
  • Multi-Grade Class B Work Life
  • Fuel-Resistant Elastomeric Seal

Product Description

PPG PR-1776M Class B Polysulfide Sealant is a low-density, two-part manganese-dioxide-cured polysulfide sealant for integral fuel-tank fillets and aircraft fuselage sealing. The low-sag thixotropic paste is applied by extrusion gun or spatula and cures at room temperature. Class B-1/2, B-2, B-4, and B-6 variants provide application lives from 0.5 to 6 hours at 25 deg C and 50% RH. The cured sealant has a typical specific gravity of 1.29, Shore A hardness of 50, and 366% elongation after the standard cure. It remains elastomeric after prolonged exposure to aircraft fuels and limited contact with phosphate-ester hydraulic fluids.

Key features

  • Low-density fuel-tank seal: A cured specific gravity of 1.29 suits weight-sensitive fuel-tank and fuselage sealing.
  • Multiple Class B work lives: B-1/2, B-2, B-4, and B-6 grades provide 0.5- to 6-hour application lives.
  • Fuel-exposed elastomeric performance: The cured sealant remains elastomeric after prolonged aircraft-fuel exposure.

Applications / Suitable for

  • Fillet sealing of integral aircraft fuel tanks.
  • Aircraft fuselage sealing.
Product Family

PRC-DESOTO PR 1776M

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Component System
Two Part
Specific Gravity
1.29
Thermal Properties
Service temperature
-54 to 121 °C
Other Properties
Storage Temperature
4.5 - 27 °C
Mechanical Properties
Elongation
366 %

Additional Information

Technical properties

As supplied / before processing

Variant-specific times are typical at 25 deg C and 50% RH.

Property Value Unit Method / condition
Part A / Part B colorBlack / Off white-As supplied
Mixed colorDark brown-After mixing
Mix ratio by weight12:100 / 10:100-B-1/2 / B-2; Part A to Part B
Base viscosity11,100 (1,100)Poise (Pa-s)Brookfield #7 at 2 rpm
Application life0.5 / 2 / 4 / 6hB-1/2 / B-2 / B-4 / B-6 at 25 deg C, 50% RH
Tack-free time<8 / <16 / <24 / <30hB-1/2 / B-2 / B-4 / B-6
Cure to 30 Shore A12 / 24 / 48 / 80hB-1/2 / B-2 / B-4 / B-6
Technical properties

After processing / final state

Values are typical after 14 days at 25 deg C and 50% RH unless otherwise stated.

Property Value Unit Method / condition
Cured specific gravity1.29-Cured 14 days at 25 deg C, 50% RH
Nonvolatile content94%Typical cured material
Ultimate cure hardness50Shore ACured 14 days at 25 deg C, 50% RH
Tensile strength263 (1,812)psi (kPa)Cured 14 days at 25 deg C, 50% RH
Elongation366%Cured 14 days at 25 deg C, 50% RH
Low-temperature flexibilityNo cracking-At -54 deg C
Service temperature range-54 to 121deg CLimited excursions up to 182 deg C