PRC-DESOTO PR 1775

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

PRC-DESOTO PR 1775

Main features

  • Non-Chromate Corrosion Barrier
  • Selectable Class B Work Life
  • Fuel-Exposed Elastomeric Seal

Product Description

PPG PR-1775 Class B Non-Chromate Corrosion-Inhibitive Sealant is a two-part, manganese-dioxide-cured polysulfide sealant for corrosion-barrier sealing of aluminum alloys and dissimilar-metal aerospace joints. The uncured material is a low-sag, thixotropic paste applied by extrusion gun or spatula and cured at room temperature. Class B-1/2 and B-2 variants provide 0.5- and 2-hour application lives at 25 deg C and 50% RH. The cured sealant has a typical Shore A hardness of 51, 420% elongation, and a service range from -54 to 121 deg C, with recurring short exposures to 182 deg C. It retains elastomeric properties after exposure to jet fuel and aviation gasoline.

Key features

  • Non-chromate corrosion barrier: The sealant forms a corrosion-inhibitive barrier on aluminum alloys and between dissimilar metals.
  • Selectable Class B work life: B-1/2 and B-2 grades provide 0.5- and 2-hour application lives at 25 deg C and 50% RH.
  • Fuel-exposed elastomeric seal: The cured material retains elastomeric properties after exposure to jet fuel and aviation gasoline.

Applications / Suitable for

  • Corrosion-barrier sealing of aluminum aerospace assemblies.
  • Sealing between dissimilar metals in aerospace assemblies.
  • Aerospace joints exposed to jet fuel or aviation gasoline.
Product Family

PRC-DESOTO PR 1775

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Component System
Two Part
Specific Gravity
1.59
Thermal Properties
Service temperature
-54 to 121 °C
Other Properties
Storage Temperature
4.5 - 27 °C
Mechanical Properties
Elongation
420 %

Additional Information

Technical properties

As supplied / before processing

Class B-1/2 and B-2 values are typical at 25 deg C and 50% RH.

Property Value Unit Method / condition
Part A / Part B colorBlack / White-As supplied
Mixed colorGray-After mixing
Mix ratio by weight12:100 / 10:100-B-1/2 / B-2; Part A to Part B
Base viscosity11,000 (1,100)Poise (Pa-s)Brookfield #7 at 2 rpm
Application life0.5 / 2hB-1/2 / B-2 at 25 deg C, 50% RH
Tack-free time<4 / <6hB-1/2 / B-2 at 25 deg C, 50% RH
Cure to 30 Shore A16 / 24hB-1/2 / B-2 at 25 deg C, 50% RH
Technical properties

After processing / final state

Values are typical after 14 days at 25 deg C and 50% RH unless otherwise stated.

Property Value Unit Method / condition
Cured specific gravity1.59-Cured 14 days at 25 deg C, 50% RH
Nonvolatile content94%Typical cured material
Ultimate cure hardness51Shore ACured 14 days at 25 deg C, 50% RH
Tensile strength495 (3,413)psi (kPa)Cured 14 days at 25 deg C, 50% RH
Elongation420%Cured 14 days at 25 deg C, 50% RH
Low-temperature flexibilityNo cracking-At -54 deg C
Service temperature range-54 to 121deg CShort recurring exposures up to 182 deg C