PLEXUS MA920

Harmonization Code : 3904.61.00.00 | Polytetrafluoroethylene plates / sheets / film / tape / strip, self-adhesive, in rolls

PLEXUS MA920

Main features

  • Fast 4-6 Minute Working Window
  • Low-Odor Structural Bonding
  • Balanced Strength and Elongation

Product Description

Plexus MA920 Methacrylate Structural Adhesive is a two-part, 10:1 low-odor system for structural bonding of thermoplastics, metals, and composites. The adhesive provides a 4-6 minute working time and reaches handling strength in 16-17 minutes, supporting rapid assembly where positioning time is limited. Typical cured tensile strength is 16.4-20.1 MPa with 30-50% elongation, and the maximum gap-fill value is 9.5 mm. Part A and Part B viscosities are 80-120 and 35-80 x 1,000 cP, respectively. MA920 is used on composites, engineered thermoplastics, coated metals, and PC-120-conditioned raw metals.

Key features

  • Fast assembly window: A 4-6 minute working time and 16-17 minute handling time support rapid part positioning and assembly.
  • Low-odor technology: The two-part methacrylate system uses odor-blocking technology for lower-odor structural bonding.
  • Strength and elongation balance: Typical cured tensile strength of 16.4-20.1 MPa is paired with 30-50% elongation.

Applications / Suitable for

  • Structural bonding of thermoplastic, metal, and composite assemblies requiring a short working window.
Product Family

PLEXUS MA920

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Component System
Two part (A / B)
Physical Properties
VOC
< 1
Other Properties
Storage Temperature
13 - 25 °C
Mechanical Properties
Elongation
30 - 50 %

Additional Information

Technical properties

As supplied / before processing

Values apply to the matched 10:1 Part A and Part B system.

Property Value Unit Method / condition
Mix ratio by volume10:1-Part A adhesive to Part B activator
Part A viscosity80-120x 1,000 cPTypical as supplied
Part B viscosity35-80x 1,000 cPTypical as supplied
Working time4-6minMixed adhesive
Handling time16-17minTypical assembly handling time
Technical properties

After processing / final state

Values are typical and do not represent universal joint performance across all substrates.

Property Value Unit Method / condition
Tensile strength16.4-20.1MPaTypical cured material
Elongation30-50%Typical cured material
Maximum gap fill9.5mmMaximum stated joint gap