PLEXUS MA590

Harmonization Code : 3904.61.00.00 | Polytetrafluoroethylene plates / sheets / film / tape / strip, self-adhesive, in rolls

PLEXUS MA590

Main features

  • 90-105 Minute Working Time
  • Up to 38.1 mm Gap Fill
  • >130% Typical Elongation

Product Description

Plexus MA590 Methacrylate Structural Adhesive provides an extended-working-time 1:1 methacrylate system for structural bonding of large composite, thermoplastic, and metal assemblies. Its 90-105 minute working time supports prolonged positioning, while the highly thixotropic consistency maintains a gap-filling bead. Typical values include a maximum gap fill of 1.5 in (38.1 mm), tensile strength of 1,880-2,750 psi, and elongation above 130%. This combination is relevant to large structures where parts must be aligned over a longer period while retaining a non-sag adhesive bead and a high-toughness cured joint.

Key features

  • Long positioning window: A 90-105 minute working time supports extended assembly of large structures.
  • High-build gap filling: The thixotropic 1:1 system supports a maximum gap fill of 1.5 in (38.1 mm).
  • Highly extensible bondline: Typical elongation exceeds 130%, with tensile strength of 1,880-2,750 psi.

Applications / Suitable for

  • Large composite, thermoplastic, and metal assemblies that require a long working window.
Product Family

PLEXUS MA590

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Component System
Two part (A / B)
Physical Properties
VOC
< 0.5
Other Properties
Storage Temperature
13 - 25 °C
Mechanical Properties
Elongation
>130 %

Additional Information

Technical properties

As supplied / before processing

Values are typical and are reported at 23 deg C unless otherwise noted.

Property Value Unit Method / condition
Mix ratio1:1-Two-part system
Working time90-105minTypical at 23 deg C
Part A viscosity140-230x 1,000 cPTypical at 23 deg C
Part B viscosity165-230x 1,000 cPTypical at 23 deg C
Maximum gap fill1.5 (38.1)in (mm)Typical joint-design value
Technical properties

After processing / final state

Values are typical and do not represent universal joint performance across all substrates.

Property Value Unit Method / condition
Tensile strength1,880-2,750psiTypical cured material at 23 deg C
Elongation>130%Typical cured material at 23 deg C
ToughnessHigh-Qualitative cured-joint characteristic

Leading Brands Trust in Our Products and Services