PLEXUS MA425

Harmonization Code : 3904.61.00.00 | Polytetrafluoroethylene plates / sheets / film / tape / strip, self-adhesive, in rolls

PLEXUS MA425

Main features

  • 30-35 Minute Working Time
  • Non-Sag Thixotropic Dispensing
  • 30-50% Typical Elongation

Product Description

Plexus MA425 Methacrylate Structural Adhesive combines a two-part 10:1 methacrylate system with a 30-35 minute working window for structural bonding of composite, thermoplastic, and metal assemblies. Its non-sag thixotropic consistency supports controlled dispensing on structural joints and helps the bead remain in place during assembly. Typical cured tensile strength is 2,565-3,315 psi with 30-50% elongation, combining load-bearing capability with joint flexibility. The product is used in transportation and marine manufacturing for composite bonding and for joining thermoplastics, coated metals, and raw metals prepared with PC120 cleaner/conditioner.

Key features

  • Extended assembly time: A 30-35 minute working window supports structural bonding of larger or more complex assemblies.
  • Non-sag dispensing: Thixotropic flow helps the adhesive remain in place during application.
  • Strength with elongation: Typical tensile strength is 2,565-3,315 psi with 30-50% elongation.

Applications / Suitable for

  • Transportation and marine structural assemblies using composites, thermoplastics, coated metals, or PC120-prepared raw metals.
Product Family

PLEXUS MA425

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Component System
Two part (A / B)
Physical Properties
VOC
<1
Other Properties
Storage Temperature
13 - 25 °C
Mechanical Properties
Elongation
30 - 50 %

Additional Information

Technical properties

As supplied / before processing

Values are typical. Viscosity and gap data are reported at 23 deg C unless otherwise noted.

Property Value Unit Method / condition
Mix ratio10:1-Two-part system
Working time30-35minMixed adhesive
Part A viscosity100-125x 1,000 cPTypical at 23 deg C
Part B viscosity35-70x 1,000 cPTypical at 23 deg C
Maximum gap fill0.375 (9.5)in (mm)Typical joint-design value
Technical properties

After processing / final state

Values are typical and do not represent universal joint performance across all substrates.

Property Value Unit Method / condition
Tensile strength2,565-3,315psiTypical cured material at 23 deg C
Elongation30-50%Typical cured material at 23 deg C
Fatigue resistanceHigh-Qualitative cured-joint characteristic

Leading Brands Trust in Our Products and Services