PLEXUS MA420W

Harmonization Code : 3904.61.00.00 | Polytetrafluoroethylene plates / sheets / film / tape / strip, self-adhesive, in rolls

PLEXUS MA420W

Main features

  • Fast 3-4 Minute Assembly
  • Rapid 13.5-Minute Strength Build
  • Wide 0.25-9.5 mm Gap Range

Product Description

Plexus MA420W is a two-part, 10:1 methacrylate adhesive for rapid structural bonding of thermoplastics, metals, and composites. At 75 deg F (23.9 deg C), it provides a 3-4 minute work time, reaches 500 psi (3.4 MPa) in 13 minutes, and reaches 1,000 psi (6.9 MPa) in 13.5 minutes. The non-sagging system fills gaps from 0.25 to 9.5 mm. Typical cured properties include 18.0-22.0 MPa tensile strength, 20-40% elongation, 75 Shore D hardness, and 25.0 MPa lap shear on aluminum.

Key features

  • 3-4 Minute Work Window: Supports rapid assembly at 75 deg F (23.9 deg C).
  • 13.5-Minute 1,000 psi Build: Develops 6.9 MPa shear strength quickly at 75 deg F.
  • 0.25-9.5 mm Gap Tolerance: Accommodates thin and thick structural joints.

Applications

Applications include rapid structural bonding of thermoplastics, metals, and composites, including transportation composite assemblies.

Product Family

PLEXUS MA420W

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Component System
Two part (A / B)
Physical Properties
VOC
<2
Other Properties
Storage Temperature
13 - 25 °C
Mechanical Properties
Elongation
20 - 40 %