PLEXUS MA2045

Harmonization Code : 3904.61.00.00 | Polytetrafluoroethylene plates / sheets / film / tape / strip, self-adhesive, in rolls

PLEXUS MA2045

Main features

  • Extended 45-50 Minute Work Window
  • Vertical Non-Sag Placement
  • Deep 38 mm Gap Bonding

Product Description

Plexus MA2045 is a two-part, 10:1 methacrylate adhesive for structural bonding of composite, thermoplastic, and metal assemblies where thick joints or vertical placement are required. The non-sagging formulation has a 45-50 minute work time at 75 deg F (23.9 deg C) and a typical gap tolerance of 0.75-38 mm. It is formulated to limit sag and slide on vertical surfaces and to avoid boiling in gaps up to 38 mm. Typical cured properties include 15.2-20.0 MPa tensile strength and 90-125% elongation.

Key features

  • 0.75-38 mm Thick-Gap Bonding: Accommodates unusually deep structural joints.
  • 45-50 Minute Work Window: Provides extended positioning time at 75 deg F (23.9 deg C).
  • Vertical Non-Sag Application: Limits sag and slide during placement on vertical surfaces.

Applications

Applications include structural bonding of composites, thermoplastics, and metals, including vertical-surface and thick-gap assemblies.

Product Family

PLEXUS MA2045

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Component System
Two part (A | B)
Physical Properties
VOC
< 1 %
Other Properties
Storage Temperature
13 - 25 °C
Mechanical Properties
Elongation
90 - 125 %

Additional Information

Technical properties

As-supplied / before-processing properties

Values are typical for the separate components and processing at 75 deg F (23.9 deg C) where stated.

Property Value Unit Method / condition
Component color - Part A / Part BOff-white / blue or blackTypical uncured
Mix ratio by volume10:1Part A to Part B
Component density - Part A0.94g/mLTypical uncured
Component density - Part B1.07g/mLTypical uncured
Component viscosity - Part A180-220x 1,000 cPTypical uncured
Component viscosity - Part B35-70x 1,000 cPTypical uncured
Work time45-50minutesAt 75 deg F (23.9 deg C)
Time to 500 psi (3.4 MPa)100-105minutesAt 75 deg F (23.9 deg C)
Technical properties

After-processing / final-state properties

Values are typical cured properties; lap-shear results apply only to the stated substrate and test method.

Property Value Unit Method / condition
Gap tolerance0.75-38mmTypical cured joint range
Hardness74Shore DTypical cured property
Tensile strength15.2-20.0MPaISO 527
Tensile modulus413-689MPaISO 527
Elongation at break90-125%ISO 527
Lap shear - aluminum16.0MPaASTM D1002; cohesive failure