PERMABOND UV7141

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

PERMABOND UV7141

Main features

  • Shadow-Area Anaerobic Cure
  • Second-Scale UV Fixture
  • High-Transmittance Glass Bonding

Product Description

Permabond UV7141 is a colorless, dual-cure methacrylate adhesive that combines rapid UV fixture with secondary anaerobic cure in shadowed areas. It is intended for ceramic-coated glass, mirrors, glass, and metal assemblies where light cannot reach the complete bondline. Typical UV fixture time ranges from 1 to 20 seconds under the listed lamp conditions, followed by anaerobic handling strength in 30 to 60 minutes and working strength in 3 to 6 hours. The cured adhesive provides 14 to 17 N/mm^2 steel-to-glass tensile strength, more than 98% light transmittance, and 60 to 70 Shore D hardness.

Key features

  • Shadow-Area Anaerobic Cure: Secondary anaerobic cure develops in bondline areas not reached by UV light.
  • Second-Scale UV Fixture: Typical UV fixture time is 1 to 20 seconds under the listed lamp conditions.
  • High-Transmittance Glass Bonding: The cured adhesive provides more than 98% light transmittance.

Applications

Applications include bonding ceramic-coated glass, mirrors, glass, and metal where UV fixture and secondary anaerobic cure are required.

Product Family

PERMABOND UV7141

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Colorless
Refractive index
1.490
Specific Gravity
1.1
Physical Properties
Viscosity
1200-1700 mPa.s
Mechanical Properties
Elongation
20-50 %
Other Properties
Storage Temperature
5 - 25 °C
Electrical Properties
Dielectric Strength
10-12 kV/mm

Additional Information

Technical properties

As-supplied / before-processing properties

Fixture time depends on lamp output, distance, and substrate transmission.

Property Value Unit Method / condition
Chemical compositionMethacrylate esterAs supplied
AppearanceColorlessAs supplied
Viscosity1,200 to 1,700mPa sAt 25 deg C; 20 rpm
Specific gravity1.1As supplied
Typical UV fixture time1 to 20secondsListed UV lamp conditions
Cure wavelength365 to 420nmMatch lamp output to the photoinitiator
Anaerobic handling time30 to 60minutesShadow-area cure
Anaerobic working strength3 to 6hoursShadow-area cure
Technical properties

After-processing / final-state properties

Values are typical cured properties for the stated methods and substrates.

Property Value Unit Method / condition
Steel-to-glass tensile strength14 to 17N/mm^2ASTM D2095-69
Tensile strength20N/mm^2ISO 37
Refractive index1.490Cured adhesive
Light transmittance>98%Cured adhesive
Elongation20 to 50%ISO 37
Hardness60 to 70Shore DISO 868
Dielectric strength10 to 12kV/mmTypical cured value
Coefficient of thermal expansion85 x 10^-6mm/mm/deg CTypical cured value