PERMABOND UV683

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

PERMABOND UV683

Main features

  • Controlled Doming and Encapsulation
  • Rapid Tack-Free UV Cure
  • High-Transmittance Cured Coating

Product Description

Permabond UV683 is a colorless UV-curable acrylate coating and doming compound for smart-card microchips and electronic-component encapsulation. Its 1,000 to 1,600 mPa s viscosity at 25 deg C supports doming application, while cure across 320 to 420 nm produces a tack-free surface. Typical tack-free time ranges from 1 to 15 seconds under the listed lamp conditions. The cured coating provides more than 98% light transmittance, 12 to 14 N/mm^2 tensile strength, more than 50% elongation, and 50 to 65 Shore D hardness for optically clear protective applications.

Key features

  • Doming-Grade Viscosity: Viscosity is 1,000 to 1,600 mPa s at 25 deg C.
  • Rapid Tack-Free Cure: Typical tack-free time is 1 to 15 seconds under the listed lamp conditions.
  • High-Transmittance Coating: The cured coating provides more than 98% light transmittance.

Applications

Applications include coating and doming, smart-card microchip coating, and encapsulation of electronic components.

Product Family

PERMABOND UV683

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Colorless
Refractive index
>1.490
Specific Gravity
1.1
Physical Properties
Viscosity
1,000-1,600 mPa.s
Mechanical Properties
Elongation
>50 %
Chemical Properties
Water Absorption
<2 %
Other Properties
Storage Temperature
2 - 7 °C
Thermal Properties
Glass Transition Temperature (Tg)
55 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Fixture time depends on lamp output, distance, and substrate transmission.

Property Value Unit Method / condition
Chemical compositionAcrylateAs supplied
AppearanceColorlessAs supplied
Viscosity1,000 to 1,600mPa sAt 25 deg C
Specific gravity1.1As supplied
Typical fixture time1 to 7secondsListed UV lamp conditions
Typical tack-free time1 to 15secondsListed UV lamp conditions
Cure wavelength320 to 420nmMatch lamp output to the photoinitiator
Technical properties

After-processing / final-state properties

Values are typical cured properties for the stated methods and substrates.

Property Value Unit Method / condition
Tensile strength12 to 14N/mm^2ISO 37
Light transmittance>98%Cured coating
Refractive index>1.490Cured coating
Elongation at break>50%ISO 37
Hardness50 to 65Shore DISO 868
Water absorption<2%ISO 62; 2 hours in boiling water