Permabond UV681 is a low-viscosity UV-curable acrylate coating for electronics protection and smart-card microchip coating. The coating has viscosity of 80 to 120 mPa s and cures to a tack-free surface. Cured values include tensile strength of 10 to 12 MPa and hardness of 50 to 65 Shore D. These characteristics support thin UV-cured protective layers requiring a dry surface and controlled cured hardness. The low-viscosity format is relevant to electronics and smart-card microchip surfaces where the complete coating area can receive UV exposure.

Key features

  • Low-Viscosity UV Coating: Viscosity is listed at 80 to 120 mPa s.
  • Tack-Free Cured Surface: UV cure produces a tack-free coating surface.
  • Cured Mechanical Profile: Cured values are 10 to 12 MPa tensile strength and 50 to 65 Shore D hardness.

Applications

Applications include electronics coating, conformal-coating protection, and smart-card microchip coating.

Product Family

PERMABOND UV681

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Colorless
Refractive index
>1.490
Specific Gravity
1.1
Physical Properties
Viscosity
80-120 mPa.s
Mechanical Properties
Elongation
>50 %
Chemical Properties
Water Absorption
<2 %
Other Properties
Storage Temperature
2 - 7 °C
Thermal Properties
Glass Transition Temperature (Tg)
55 °C

Additional Information

Technical properties

After-processing / final-state properties

Property Value Unit Method / condition
Cured coating surfaceTack-freeUV-cured coating characteristic
Tensile strength10 to 12MPaCured coating
Hardness50 to 65Shore DCured coating