PERMABOND UV648

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

PERMABOND UV648

Main features

  • Non-Drip Application Control
  • UV-Stabilized Plastic Bonding
  • Colorless High-Elongation Cure

Product Description

Permabond UV648 is a single-part, non-drip urethane-methacrylate adhesive for UV bonding of acrylic, UV-stabilized plastics, glass, and metals. Its long-wavelength photoinitiator supports cure through UV-stabilized plastic, while the clear formulation produces a colorless bond. At 25 deg C, viscosity is 20,000 to 40,000 mPa s at 20 rpm, and typical fixture time is 2 to 10 seconds under the listed lamp conditions. Cured properties include more than 70% elongation, 50 to 65 Shore D hardness, and overlap shear values above 7 N/mm^2 on polycarbonate and above 4 N/mm^2 on acrylic and PET.

Key features

  • Non-Drip Application Control: High shear-dependent viscosity limits flow before UV cure.
  • UV-Stabilized Plastic Cure: A long-wavelength photoinitiator supports cure through UV-stabilized plastics.
  • Colorless Flexible Bond: The cured adhesive is colorless and provides more than 70% elongation.

Applications

Applications include bonding acrylic, UV-stabilized plastics, glass, metals, polycarbonate, and PET where UV transmission is adequate.

Product Family

PERMABOND UV648

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Colorless, clear
Refractive index
>1.490
Specific Gravity
1.1
Physical Properties
Viscosity
20,000-40,000 | 120,000-180,000 mPa.s
Mechanical Properties
Elongation
>70 %
Electrical Properties
Dielectric Strength
25-30 kV/mm
Chemical Properties
Water Absorption
<3.5 %
Other Properties
Storage Temperature
5 - 25 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Fixture time depends on lamp output, distance, and substrate transmission.

Property Value Unit Method / condition
Chemical compositionUrethane methacrylateAs supplied
AppearanceColorless, clearAs supplied
Viscosity20,000 to 40,000mPa sAt 25 deg C; 20 rpm
Viscosity120,000 to 180,000mPa sAt 25 deg C; 2.5 rpm
Specific gravity1.1As supplied
Typical fixture time2 to 10secondsListed UV lamp conditions
Cure wavelength365 to 420nmMatch lamp output to the photoinitiator
Technical properties

After-processing / final-state properties

Values are typical cured properties for the stated methods and substrates.

Property Value Unit Method / condition
Overlap shear strength - polycarbonate>7N/mm^2ISO 4587; substrate failure observed
Overlap shear strength - acrylic>4N/mm^2ISO 4587
Overlap shear strength - PET>4N/mm^2ISO 4587; substrate failure observed
Tensile strength11N/mm^2ISO 37
Refractive index1.490Cured adhesive
Elongation at break>70%ISO 37
Hardness50 to 65Shore DISO 868
Dielectric strength25 to 30kV/mmTypical cured value

Leading Brands Trust in Our Products and Services