PERMABOND UV645

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

PERMABOND UV645

Main features

  • High-Viscosity Controlled Application
  • Fast 2 to 10 Second Fixture
  • Flexible Plastic-Bonding Cure

Product Description

Permabond UV645 is a single-part, high-viscosity methacrylate adhesive for fast UV bonding of plastics, including acrylic and polycarbonate, with additional use on glass and metals. The clear formulation cures across 365 to 420 nm and provides typical fixture times from 2 to 10 seconds under the listed lamp conditions. At 25 deg C, viscosity is 8,000 to 10,000 mPa s at 20 rpm. The cured adhesive combines more than 70% elongation with 50 to 65 Shore D hardness and measured shear strength on polycarbonate, PVC, PC/ABS, and acrylic.

Key features

  • High-Viscosity Application Control: Viscosity is 8,000 to 10,000 mPa s at 25 deg C and 20 rpm.
  • Fast UV Fixture: Typical fixture time is 2 to 10 seconds under the listed lamp conditions.
  • Flexible Cured Bond: The cured adhesive provides more than 70% elongation with 50 to 65 Shore D hardness.

Applications

Applications include bonding acrylic, polycarbonate, PVC, PC/ABS, glass, and metal, plus supported UV-curable sealing applications.

Product Family

PERMABOND UV645

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Colorless, clear
Refractive index
>1.490
Specific Gravity
1.1
Physical Properties
Viscosity
8,000-10,000 | 30,000-60,000 mPa.s
Mechanical Properties
Elongation
>70 %
Electrical Properties
Dielectric Strength
25-30 kV/mm
Chemical Properties
Water Absorption
<5 %
Other Properties
Storage Temperature
5 - 25 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Fixture time depends on lamp output, distance, and substrate transmission.

Property Value Unit Method / condition
Chemical compositionMethacrylate esterAs supplied
AppearanceColorless, clearAs supplied
Viscosity8,000 to 10,000mPa sAt 25 deg C; 20 rpm
Viscosity30,000 to 60,000mPa sAt 25 deg C; 2.5 rpm
Specific gravity1.1As supplied
Typical fixture time2 to 10secondsListed UV lamp conditions
Cure wavelength365 to 420nmMatch lamp output to the photoinitiator
Technical properties

After-processing / final-state properties

Values are typical cured properties for the stated methods and substrates.

Property Value Unit Method / condition
Overlap shear strength - polycarbonate>9N/mm^2ISO 4587; substrate failure observed
Overlap shear strength - PVC>5N/mm^2ISO 4587
Overlap shear strength - PC/ABS>7N/mm^2ISO 4587; substrate failure observed
Overlap shear strength - acrylic>1.5N/mm^2ISO 4587; substrate failure observed
Tensile strength11N/mm^2ISO 37
Elongation at break>70%ISO 37
Hardness50 to 65Shore DISO 868
Dielectric strength25 to 30kV/mmTypical cured value