PERMABOND UV643

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

PERMABOND UV643

Main features

  • Sub-Second High-Intensity Fixture
  • Thixotropic Rigid-Plastic Bonding
  • Hot-Wet Strength Retention

Product Description

Permabond UV643 is a thixotropic, extremely fast urethane-acrylate adhesive for UV bonding of rigid plastics and metal-to-plastic assemblies. It cures tack-free across 365 to 420 nm and bonds polycarbonate, PMMA, PETG, PET, ABS, and rigid PVC under the specified process conditions. Typical fixture time is under 1 second with the listed 330 mW/cm^2 mercury lamp or 400 nm, 150 mW/cm^2 LED, and 19 seconds at 0.1 mW/cm^2. Cured data include 23 N/mm^2 tensile strength, 50% elongation, and retained polycarbonate shear strength after four weeks at 85 deg C and 85% RH.

Key features

  • Thixotropic Application Control: Viscosity is 2,000 mPa s at 20 rpm and 17,600 mPa s at 2 rpm.
  • Sub-Second High-Intensity Fixture: Typical fixture time is under 1 second with the listed high-intensity UV lamp conditions.
  • Hot-Wet Strength Retention: Polycarbonate shear strength remained 13 N/mm^2 after four weeks at 85 deg C and 85% RH.

Applications

Applications include fast bonding of PC, PMMA, PETG, PET, ABS, rigid PVC, and supported metal-to-plastic combinations.

Product Family

PERMABOND UV643

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Pale yellow (colourless when cured)
Specific Gravity
1.0
Physical Properties
Viscosity
2000 | 17,600 mPa.s
Mechanical Properties
Elongation
50 %
Chemical Properties
Water Absorption
5 %
Other Properties
Storage Temperature
5 - 25 °C
Thermal Properties
Glass Transition Temperature (Tg)
83 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Fixture time depends on lamp output, distance, and substrate transmission.

Property Value Unit Method / condition
Chemical compositionUrethane acrylateAs supplied
AppearancePale yellowColorless when cured
Viscosity2,000mPa sAt 25 deg C; 20 rpm
Viscosity17,600mPa sAt 25 deg C; 2 rpm
Specific gravity1.0As supplied
Typical fixture time<1 to 19secondsListed UV lamp conditions
Cure wavelength365 to 420nmMatch lamp output to the photoinitiator
Technical properties

After-processing / final-state properties

Values are typical cured properties for the stated methods and substrates.

Property Value Unit Method / condition
Overlap shear strength - polycarbonate13N/mm^2Substrate failure observed
Overlap shear strength - acrylic7N/mm^2Typical cured value
Overlap shear strength - aluminum to PC10N/mm^2Typical cured value
Tensile strength23N/mm^2ASTM D638
Elongation at break50%ASTM D638
Elastic modulus1.2GPaASTM D638
Hardness65Shore DISO 868
Polycarbonate shear after hot-wet aging13N/mm^24 weeks at 85 deg C and 85% RH; tested at 23 deg C