PERMABOND UV640

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

PERMABOND UV640

Main features

  • Fast Low-Power UV Cure
  • High-Elongation Plastic Bonding
  • Clear Polycarbonate Assembly

Product Description

Permabond UV640 is a single-part, medium-viscosity methacrylate adhesive developed for rapid UV bonding of plastics, including polycarbonate and acrylic. The clear liquid cures on demand across 365 to 420 nm, with typical fixture times from 2 to 10 seconds under the listed lamp conditions. At 25 deg C, viscosity is 3,000 to 5,000 mPa s at 20 rpm. The cured adhesive combines 13 N/mm^2 tensile strength with 110% elongation and 55 to 75 Shore D hardness, supporting plastic assemblies and joints between substrates with different coefficients of thermal expansion.

Key features

  • Fast Low-Power UV Cure: Typical fixture time is 2 to 10 seconds under the listed UV lamp conditions.
  • Medium-Viscosity Placement: Viscosity is 3,000 to 5,000 mPa s at 25 deg C and 20 rpm.
  • High-Elongation Cured Bond: The cured adhesive reaches 110% elongation with 13 N/mm^2 tensile strength.

Applications

Applications include bonding polycarbonate, acrylic, and other supported plastics, including assemblies with different coefficients of thermal expansion.

Product Family

PERMABOND UV640

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Colorless, clear
Refractive index
>1.490
Specific Gravity
1.1
Physical Properties
Viscosity
3,000-5,000 | 12,000-25,000 mPa.s
Mechanical Properties
Elongation
110 %
Electrical Properties
Dielectric Strength
25-30 kV/mm
Chemical Properties
Water Absorption
<5 %
Other Properties
Storage Temperature
5 - 25 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Fixture time depends on lamp output, distance, and substrate transmission.

Property Value Unit Method / condition
Chemical compositionMethacrylate esterAs supplied
AppearanceColorless, clearAs supplied
Viscosity3,000 to 5,000mPa sAt 25 deg C; 20 rpm
Viscosity12,000 to 25,000mPa sAt 25 deg C; 2.5 rpm
Specific gravity1.1As supplied
Typical fixture time2 to 10secondsListed UV lamp conditions
Cure wavelength365 to 420nmMatch lamp output to the photoinitiator
Technical properties

After-processing / final-state properties

Values are typical cured properties for the stated methods and substrates.

Property Value Unit Method / condition
Overlap shear strength - polycarbonate>9N/mm^2ISO 4587; substrate failure observed
Overlap shear strength - acrylic>1.5N/mm^2ISO 4587; substrate failure observed
Tensile strength13N/mm^2ISO 37
Elongation at break110%ISO 37
Hardness55 to 75Shore DISO 868
Dielectric strength25 to 30kV/mmTypical cured value
Dielectric constant41 MHz at 25 deg C
Water absorption<5%ISO 62; 2 hours in boiling water