PERMABOND UV630

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

PERMABOND UV630

Main features

  • Low-Viscosity Plastic Bonding
  • Fast 365 to 420 nm Cure
  • High-Elongation Cured Bond

Product Description

Permabond UV630 is a single-part, low-viscosity methacrylate adhesive for fast UV bonding of plastics, including polycarbonate. The clear liquid has a typical viscosity of 250 mPa s at 25 deg C and cures across 365 to 420 nm. Depending on lamp output and substrate transmission, fixture time on acrylic ranges from 10 seconds with a 4 mW/cm^2 battery lamp to 2 seconds with a 300 mW/cm^2 light guide. The cured adhesive combines typical tensile strength of 14 N/mm^2 with 110% elongation and high shear and impact resistance for assemblies using substrates with different coefficients of thermal expansion.

Key features

  • Low-Viscosity Plastic Bonding: A 250 mPa s viscosity supports controlled application to plastic joints.
  • Fast 365 to 420 nm Cure: Fixtures on acrylic in 2 to 10 seconds under the stated lamp conditions.
  • High-Elongation Cured Bond: Provides 110% typical elongation with high shear and impact resistance.

Applications

Applications include plastic bonding, polycarbonate assembly, and joints that combine substrates with different coefficients of thermal expansion.

Product Family

PERMABOND UV630

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Colorless, clear
Refractive index
>1.490
Specific Gravity
1.1
Physical Properties
Viscosity
200-300 mPa.s
Mechanical Properties
Elongation
110 %
Electrical Properties
Dielectric Strength
25-30 kV/mm
Chemical Properties
Water Absorption
<3.5 %
Other Properties
Storage Temperature
5 - 25 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Fixture time depends on lamp power, spectral output, distance, and substrate transmission.

Property Value Unit Method / condition
Chemical compositionMethacrylate esterAs supplied
AppearanceColorless, clearAs supplied
Viscosity250mPa sAt 25 deg C; 20 rpm
Specific gravity1.1As supplied
Fixture time on acrylic10seconds4 mW/cm^2 battery lamp
Fixture time on acrylic4seconds100 mW/cm^2 LED lamp
Fixture time on acrylic2seconds300 mW/cm^2 UV light guide
Cure wavelength365 to 420nmMatch lamp output to the photoinitiator
Technical properties

After-processing / final-state properties

Strength and dielectric values are typical cured results for the stated methods.

Property Value Unit Method / condition
Overlap shear - polycarbonate>9N/mm^2ISO 4587; substrate failure observed
Overlap shear - acrylic>1.5N/mm^2ISO 4587
Tensile strength14N/mm^2ISO 37
Refractive index>1.490Cured adhesive
Elongation at break110%ISO 37
Hardness60Shore DISO 868
Dielectric strength25 to 30kV/mmTypical cured value
Water absorption<3.5%ISO 62; 2 hours in boiling water

Leading Brands Trust in Our Products and Services