PERMABOND UV6260

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

PERMABOND UV6260

Main features

  • Filtered-Light UV Curing
  • Tack-Free Surface Cure
  • High-Elongation Plastic Bonding

Product Description

Permabond UV6260 is a thixotropic, extremely fast UV-curable urethane acrylate adhesive for metals, glass, and rigid plastics when the substrate filters the curing light. The pale-yellow liquid cures colorless and tack-free across 365 to 420 nm. On glass, typical fixture time is below 1 second with a 395 nm, 150 mW/cm^2 LED and 6 seconds at 0.1 mW/cm^2, subject to lamp and substrate conditions. Cured data include overlap shear above 11 N/mm^2 on polycarbonate with substrate failure, 205% elongation, and 60 Shore D hardness.

Key features

  • Filtered-Light UV Cure: Cures across 365 to 420 nm for substrates that filter the curing light.
  • Tack-Free Surface Cure: Produces a tack-free surface after adequate UV exposure.
  • Rigid-Plastic Bond Strength: Provides substrate-failure shear results on polycarbonate, acrylic, PETG, and PVC-to-PC joints.

Applications

Applications include bonding colored glass, metals, polycarbonate, PMMA, PETG, PET, ABS, and rigid PVC where curing-light transmission is adequate.

Product Family

PERMABOND UV6260

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Pale yellow (colourless when cured)
Specific Gravity
1.0
Physical Properties
Viscosity
45,000 | 17,000 mPa.s
Mechanical Properties
Elongation
205 %
Electrical Properties
Dielectric Strength
12 kV/mm
Chemical Properties
Water Absorption
2 %
Other Properties
Storage Temperature
5 - 25 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Fixture time depends on lamp power, spectral output, distance, and substrate transmission.

Property Value Unit Method / condition
Chemical compositionUrethane acrylateAs supplied
AppearancePale yellowColorless when cured
Viscosity45,000mPa sAt 25 deg C; 2 rpm
Viscosity17,000mPa sAt 25 deg C; 20 rpm
Specific gravity1.0As supplied
Fixture time on glass<1second395 nm LED at 150 mW/cm^2
Fixture time on glass6seconds395 nm LED at 0.1 mW/cm^2
Cure wavelength365 to 420nmMatch lamp output to the photoinitiator
Technical properties

After-processing / final-state properties

Strength values are typical cured results for the stated substrate combinations and methods.

Property Value Unit Method / condition
Overlap shear - polycarbonate>11N/mm^2ISO 4587; substrate failure observed
Overlap shear - acrylic>6N/mm^2ISO 4587; substrate failure observed
Overlap shear - PETG>9N/mm^2ISO 4587; substrate failure observed
Overlap shear - PVC to PC>10N/mm^2ISO 4587; substrate failure observed
Block shear - aluminum to glass10 to 14N/mm^2ASTM D-4501
Tensile strength10N/mm^2ISO 527
Elongation at break205%ISO 527
Hardness60Shore DISO 868

Leading Brands Trust in Our Products and Services