PERMABOND UV625

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

PERMABOND UV625

Main features

  • Non-Drip Vertical Bonding
  • Larger-Gap UV Application
  • Flexible Impact-Resistant Cure

Product Description

Permabond UV625 is a single-part, non-drip methacrylate gel for UV-curing glass-to-metal bonds and seals. Its gel-like, shear-dependent viscosity supports vertical surfaces and larger gaps while limiting flow before cure. Typical fixture time ranges from 5 seconds with a 4 mW/cm^2 battery lamp to 1 second with a 30 W/cm^2 light guide across a 365 to 400 nm cure range. The cured adhesive is tough and flexible, with typical tensile strength of 16 N/mm^2, elongation above 60%, and steel-to-glass tensile strength of 6 to 10 N/mm^2.

Key features

  • Non-Drip Vertical Application: Gel-like rheology limits flow on vertical bonding and sealing surfaces.
  • Larger-Gap UV Bonding: Good depth of cure supports larger-gap UV applications.
  • Flexible Impact-Resistant Cure: Cures to a tough, flexible bond with good impact resistance.

Applications

Applications include glass-to-metal bonding and sealing, vertical assemblies, and UV-curable joints with larger gaps.

Product Family

PERMABOND UV625

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Colorless gel
Refractive index
>1.490
Specific Gravity
1.0
Physical Properties
Viscosity
30,000-55,000 mPa.s
Mechanical Properties
Elongation
>60 %
Electrical Properties
Dielectric Strength
12 kV/mm
Chemical Properties
Water Absorption
<4 %
Other Properties
Storage Temperature
5 - 25 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Fixture time depends on lamp power, spectral output, distance, and substrate transmission.

Property Value Unit Method / condition
Chemical compositionMethacrylate esterAs supplied
AppearanceColorless gelAs supplied
Viscosity30,000 to 55,000mPa sAt 25 deg C; 20 rpm
Viscosity120,000 to 250,000mPa sAt 25 deg C; 2.5 rpm
Specific gravity1.0As supplied
Fixture time5seconds4 mW/cm^2 battery lamp
Fixture time2seconds100 mW/cm^2 LED lamp
Cure wavelength365 to 400nmMatch lamp output to the photoinitiator
Technical properties

After-processing / final-state properties

Strength and dielectric values are typical cured results for the stated methods.

Property Value Unit Method / condition
Steel-to-glass tensile strength6 to 10N/mm^2ASTM D-2095-69
Tensile strength16N/mm^2ISO 37
Refractive index>1.490Cured adhesive
Elongation>60%ISO 37
Hardness60 to 70Shore DISO 868
Dielectric strength12kV/mmTypical cured value
Dielectric constant41 MHz at 25 deg C
Water absorption<4%ISO 62; 2 hours in boiling water