PERMABOND UV620

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

PERMABOND UV620

Main features

  • Optically Clear Glass Bonding
  • Yellowing-Resistant Cured Appearance
  • Rapid Low-Power Lamp Cure

Product Description

Permabond UV620 is a single-part, optically clear methacrylate adhesive for UV-curing glass, crystal, and decorative assemblies. The colorless liquid has a typical viscosity of 2,200 to 2,900 mPa s at 25 deg C and is formulated to resist yellowing for appearance-sensitive bonds. Typical fixture time is 5 seconds with a 4 mW/cm^2 battery lamp and 1 second with a 30 W/cm^2 light guide, subject to lamp output and substrate transmission. The cured material has a refractive index above 1.490, typical tensile strength of 16 N/mm^2, and elongation above 80%.

Key features

  • Optically Clear Bondline: Supports appearance-sensitive glass and crystal assemblies with a cured refractive index above 1.490.
  • Yellowing-Resistant Appearance: Resists yellowing in appearance-sensitive decorative assemblies.
  • Rapid Optically Clear Cure: Fixtures in 5 seconds with a 4 mW/cm^2 battery lamp under stated conditions.

Applications

Applications include bonding glass, crystal, glass furniture, decorative ornaments, and other appearance-sensitive glass objects.

Product Family

PERMABOND UV620

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Colorless, clear
Refractive index
>1.490
Specific Gravity
1.0
Physical Properties
Viscosity
2,200-2,900 mPa.s
Mechanical Properties
Elongation
>80 %
Electrical Properties
Dielectric Strength
12 kV/mm
Chemical Properties
Water Absorption
<4 %
Other Properties
Storage Temperature
5 - 25 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Fixture time depends on lamp power, spectral output, distance, and substrate transmission.

Property Value Unit Method / condition
Chemical compositionMethacrylate esterAs supplied
AppearanceColorless, clearAs supplied
Viscosity2,200 to 2,900mPa sAt 25 deg C; 20 rpm
Specific gravity1.0As supplied
Fixture time5seconds4 mW/cm^2 battery lamp
Fixture time2seconds100 mW/cm^2 LED lamp
Fixture time1second30 W/cm^2 UV light guide
Cure wavelength365 to 400nmMatch lamp output to the photoinitiator
Technical properties

After-processing / final-state properties

Strength and optical values are typical cured results for the stated methods.

Property Value Unit Method / condition
Steel-to-glass tensile strength9 to 10N/mm^2ASTM D-2095-69
Tensile strength16N/mm^2ISO 37
Refractive index>1.490Cured adhesive
Elongation>80%ISO 37
Hardness60 to 75Shore DISO 868
Dielectric strength12kV/mmTypical cured value
Dielectric constant41 MHz at 25 deg C
Water absorption<4%ISO 62; 2 hours in boiling water