PERMABOND UV610

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

PERMABOND UV610

Main features

  • Fast Low-Power UV Cure
  • High-Strength Glass-Metal Bonding
  • Solvent-Free Cure-On-Demand Processing

Product Description

Permabond UV610 is a single-part, 100% solids methacrylate adhesive developed for UV-curing glass-to-metal assemblies. Its translucent, 600 to 1,300 mPa s viscosity supports direct bottle application or controlled automated dispensing. Depending on lamp output and substrate transmission, typical fixture time ranges from 10 seconds with a 4 mW/cm^2 battery lamp to 1 second with a 30 W/cm^2 light guide across a 365 to 400 nm cure range. The cured adhesive provides typical steel-to-glass tensile strength of 13 to 16 N/mm^2 and 95% elongation, supporting glass furniture and high-strength edge joints.

Key features

  • Fast Low-Power UV Cure: Fixtures in 10 seconds with a 4 mW/cm^2 battery lamp under stated conditions.
  • High-Strength Glass-to-Metal Bonding: Provides typical steel-to-glass tensile strength of 13 to 16 N/mm^2.
  • 100% Solids Formulation: Uses a solvent-free, single-part formulation for cure-on-demand processing.

Applications

Applications include glass-to-metal bonding, glass furniture assembly, and high-strength glass edge joints with direct UV exposure.

Product Family

PERMABOND UV610

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Translucent
Refractive index
>1.490
Specific Gravity
1.0
Physical Properties
Viscosity
600-1300 mPa.s
Mechanical Properties
Elongation
95 %
Electrical Properties
Dielectric Strength
12 kV/mm
Chemical Properties
Water Absorption
3 %
Other Properties
Storage Temperature
5 - 25 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Fixture time depends on lamp power, spectral output, distance, and substrate transmission.

Property Value Unit Method / condition
Chemical compositionMethacrylate esterAs supplied
AppearanceTranslucentAs supplied
Viscosity600 to 1,300mPa sAt 25 deg C; 20 rpm
Specific gravity1.0As supplied
Fixture time10seconds4 mW/cm^2 battery lamp
Fixture time2seconds100 mW/cm^2 LED lamp
Fixture time1second30 W/cm^2 UV light guide
Cure wavelength365 to 400nmMatch lamp output to the photoinitiator
Technical properties

After-processing / final-state properties

Strength values are typical cured results for the stated substrate and test methods.

Property Value Unit Method / condition
Steel-to-glass tensile strength13 to 16N/mm^2ASTM D-2095-69
Tensile strength17N/mm^2ISO 37
Refractive index>1.490Cured adhesive
Elongation95%ISO 37
Hardness65 to 75Shore DISO 868
Dielectric strength12kV/mmTypical cured value
Dielectric constant41 MHz at 25 deg C
Water absorption3%ISO 62; 2 hours in boiling water