PERMABOND TA4811

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

PERMABOND TA4811

Main features

  • 1:1 toughened methacrylate chemistry
  • Fast room-temperature cure
  • Durable structural performance

Product Description

PERMABOND TA4811 is a two-part, 1:1 toughened methacrylate structural adhesive designed for bonding thermoplastics, thermosets, metals, and composites. The adhesive develops strong bonds to a wide range of substrates, including as-received metal surfaces without surface preparation. TA4811 cures rapidly at room temperature and features thixotropic, non-sag characteristics that support easy dispensing through static mixers while maintaining gap-filling capability. The cured adhesive offers high shear and peel strength, good impact resistance, chemical resistance, and durability in demanding industrial environments.

Key features

  • 1:1 toughened methacrylate chemistry: Simplifies mixing and dispensing while supporting reliable structural bonding.
  • Fast room-temperature cure: Provides a 4-6 minute working time, 10-15 minute fixture time, and full cure within 24 hours.
  • Durable structural performance: Delivers high shear strength along with good impact, chemical, and environmental resistance.

Applications / Suitable for

  • Bonding thermoplastics
  • Bonding thermoset materials
  • Metal assembly applications
  • Composite component bonding
  • Industrial assemblies requiring gap-filling and non-sag adhesive performance
Product Family

PERMABOND TA4811

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Off-white | Black
Component System
TA4811 A | TA4811 B
Density (g)
1.02 | 1.04 g/cm3
Mix Ratio
1:1
Other Properties
Maximum gap fill
2 mm
Curing Conditions
Fixture Time
10-15 minutes
Mechanical Properties
Elongation
15-20 %
Thermal Properties
Thermal Conductivity
0.1 W/m.K
Electrical Properties
Dielectric Strength
30-50 kV/mm
Volume Resistivity
2 x 10¹³ Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uncured adhesive and processing properties.

Property Value Unit Method / condition
Mix ratio 1:1 - Part A : Part B
Mixed viscosity 90,000-100,000 cP @ 25°C
Working time 4-6 minutes Typical
Fixture time 10-15 minutes Typical
Maximum gap fill 2 mm Typical
Full cure 24 hours Room temperature
Technical properties

After-processing / final-state properties

Typical cured adhesive performance properties.

Property Value Unit Method / condition
Shear strength (steel) 3,500-4,500 psi ASTM D1002
Shear strength (aluminum) 3,000-4,000 psi ASTM D1002
Tensile strength 4,200 psi DIN 53283
Peel strength 15-20 pli Typical
Elongation 15-20 % Typical
Thermal conductivity 0.1 W/m·K ASTM C177

Leading Brands Trust in Our Products and Services