Permabond TA4611 is a two-part, 1:1 toughened acrylic adhesive developed for polypropylene and polyethylene without primer or costly surface treatment. Its microbead-free formulation is intended for joints with smaller gaps while retaining compatibility with selected metals and composites. The transparent to pale-yellow mixed adhesive supports a maximum gap of 0.5 mm. At 23 deg C, typical pot life is 4 to 6 minutes, fixture strength develops in 10 to 16 minutes, and handling strength in 40 to 50 minutes. Cured shear results include 14 N/mm^2 on carbon fiber, 13 N/mm^2 on epoxy FRP, and 8 N/mm^2 on HDPE.

Key features

  • Microbead-Free Small-Gap Bonding: Supports joints up to the 0.5 mm maximum gap.
  • Primer-Free Polyolefins: Bonds polypropylene and polyethylene without primer or costly surface treatment.
  • Dissimilar-Material Assembly: Supports selected metal, composite, and polyolefin substrate combinations.

Applications

Applications include smaller-gap bonding of polypropylene and polyethylene, plus selected metal, composite, and dissimilar-material assemblies.

Product Family

PERMABOND TA4611

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Translucent / Transparent
Component System
TA4611 A / TA4611 B
Mix Ratio
1:1
Pot Life
4-6 minutes
Specific Gravity
1.0 / 1.0
Other Properties
Maximum gap fill
0.5 mm
Storage Temperature
2 - 7 | 5 - 25 °C
Curing Conditions
Fixture Time
10-16 minutes

Additional Information

Technical properties

As-supplied / before-processing properties

Values identify the separate Part A and Part B components or the mixed adhesive, as stated.

Property Value Unit Method / condition
Part A viscosity20,000 to 30,000mPa sAt 25 deg C
Part B viscosity10,000 to 15,000mPa sAt 25 deg C
Specific gravity1.0Part A and Part B
Mix ratio1:1Part A to Part B
Maximum gap fill0.5mmMicrobead-free formulation
Pot life4 to 6minutes2 g + 2 g at 23 deg C
Fixture time10 to 16minutes0.1 N/mm^2 shear strength at 23 deg C
Handling time40 to 50minutes0.3 N/mm^2 shear strength at 23 deg C
Technical properties

After-processing / final-state properties

Strength values are typical cured results for the listed substrates and ISO 4587 test method.

Property Value Unit Method / condition
Shear strength - polypropylene>8N/mm^2ISO 4587; substrate failure observed
Shear strength - polyethylene>7N/mm^2ISO 4587; substrate failure observed
Shear strength - HDPE8N/mm^2ISO 4587
Shear strength - mild steel11N/mm^2ISO 4587
Shear strength - stainless steel9N/mm^2ISO 4587
Shear strength - aluminum to PP8N/mm^2ISO 4587
Shear strength - carbon fiber14N/mm^2ISO 4587
Shear strength - epoxy FRP13N/mm^2ISO 4587