PERMABOND TA4605

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

PERMABOND TA4605

Main features

  • Primer-Free Polyolefin Bonding
  • Controlled 1 mm Gap Filling
  • Fast Handling-Strength Development

Product Description

Permabond TA4605 is a two-part, 1:1 toughened acrylic adhesive for bonding low-surface-energy plastics, including polypropylene and polyethylene, without primer or surface treatment. The thixotropic system also bonds metals and composites and supports dissimilar-material assemblies. Microparticles control a maximum gap of 1 mm, while a 2 to 4 minute pot life at 23 deg C provides a defined assembly window. Fixture strength develops in 5 to 10 minutes, handling strength in 20 to 25 minutes, and full cure in 24 hours at 23 deg C. Cured shear results include 15 N/mm^2 on HDPE and 6 N/mm^2 on aluminum-to-PE joints.

Key features

  • Primer-Free Polyolefin Bonding: Bonds polypropylene and polyethylene without a separate primer or surface treatment.
  • Controlled 1 mm Gap: Microparticles help maintain the 1 mm maximum gap during assembly.
  • Fast Handling Development: Reaches typical handling strength in 20 to 25 minutes at 23 deg C.

Applications

Applications include bonding polypropylene, polyethylene, metals, composites, and dissimilar-material assemblies.

Product Family

PERMABOND TA4605

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Off-white / Almost colorless
Component System
TA4605 A / TA4605 B
Mix Ratio
1:1
Pot Life
2-4 minutes
Specific Gravity
1.0 / 1.0
Other Properties
Maximum gap fill
1 mm
Storage Temperature
2 - 7 | 5 - 25 °C
Curing Conditions
Fixture Time
5-10 minutes

Additional Information

Technical properties

As-supplied / before-processing properties

Values identify the separate Part A and Part B components or the mixed adhesive, as stated.

Property Value Unit Method / condition
Part A viscosity150,000 to 400,000mPa sAt 25 deg C; thixotropic paste
Part B viscosity20,000 to 30,000mPa sAt 25 deg C
Specific gravity1.0Part A and Part B
Mix ratio1:1Part A to Part B
Maximum gap fill1mmContains microparticles for gap control
Pot life2 to 4minutes2 g + 2 g at 23 deg C
Fixture time5 to 10minutes0.1 N/mm^2 shear strength at 23 deg C
Handling time20 to 25minutes0.3 N/mm^2 shear strength at 23 deg C
Technical properties

After-processing / final-state properties

Strength values are typical cured results for the listed substrates and ISO 4587 test method.

Property Value Unit Method / condition
Shear strength - polypropylene>8N/mm^2ISO 4587; substrate failure observed
Shear strength - polyethylene>7N/mm^2ISO 4587; substrate failure observed
Shear strength - HDPE15N/mm^2ISO 4587
Shear strength - aluminum to PE6N/mm^2ISO 4587
Shear strength - PTFE1.5N/mm^2ISO 4587
Shear strength - ABS>4N/mm^2ISO 4587; substrate failure observed
Shear strength - polycarbonate>5N/mm^2ISO 4587; substrate failure observed
Shear strength - EPDM>3.5N/mm^2ISO 4587; substrate failure observed